A clothing treatment and softener technology, applied in fiber treatment, textiles and papermaking, etc., can solve the problems of the clothes being slippery, static-removing and sterilizing effect, etc., and achieve the effect of excellent anti-static performance, maintaining water absorption capacity, and not easy to stick to dust.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0009] This embodiment provides a softener for treating clothes, which contains the following components in parts by mass: 12 parts of ester quaternary ammonium salt, 1 part of polyacrylate emulsion, 3 parts of sodium myristate sarcosinate, and 0.5 part of polyethyleneimine , 0.5 parts of silicone oil, 0.4 parts of stearic acid, 0.02 parts of preservatives, 0.05 parts of natural essence, 0.01 parts of dye, 145 parts of deionized water.
[0010] A softener for treating clothes, the preparation method of which is as follows: add deionized water into a stirrer, heat up to 40°C, then add ester quaternary ammonium salt, sodium myristate sarcosinate and polyethyleneimine, and stir for 30 minutes; Then add polyacrylate emulsion, silicone oil and stearic acid, stir for 20 minutes, add preservatives and dyes, stir evenly, cool down to 30°C, add natural essence, mix evenly to get the finished product.
[0011] Use the fabric softener provided in this example to treat the towel that has ...
Embodiment 2
[0013] This embodiment provides a softener for treating clothes, which contains the following components in parts by mass: 14 parts of ester quaternary ammonium salt, 1.3 parts of polyacrylate emulsion, 4.5 parts of sodium myristate, and 0.62 parts of polyethyleneimine , 1.3 parts of silicone oil, 0.9 parts of stearic acid, 0.04 parts of preservatives, 0.08 parts of natural essence, 0.015 parts of dyes, 148 parts of deionized water.
[0014] A softener for treating clothes, the preparation method of which is as follows: add deionized water into a stirrer, heat up to 50°C, then add ester quaternary ammonium salt, sodium myristate sarcosinate and polyethyleneimine, and stir for 40 minutes; Then add polyacrylate emulsion, silicone oil and stearic acid, stir for 30 minutes, add preservatives and dyes, stir evenly, cool down to 35°C, add natural essence, mix evenly to get the finished product.
[0015] Treating the sweater with the fabric softener provided in this embodiment can ma...
Embodiment 3
[0017] This embodiment provides a softener for treating clothes, which contains the following components in parts by mass: 17 parts of ester quaternary ammonium salt, 2 parts of polyacrylate emulsion, 8 parts of sodium myristate sarcosinate, and 0.75 parts of polyethyleneimine , 3 parts of silicone oil, 2 parts of stearic acid, 0.065 parts of preservatives, 0.1 parts of natural flavor, 0.022 parts of dye, 155 parts of deionized water.
[0018] A softener for treating clothes, the preparation method of which is as follows: add deionized water into a stirrer, heat up to 45°C, then add ester quaternary ammonium salt, sodium myristate sarcosinate and polyethyleneimine, and stir for 35 minutes; Then add polyacrylate emulsion, silicone oil and stearic acid, stir for 25 minutes, add preservatives and dyes, stir evenly, cool down to 32°C, add natural essence, mix evenly to get the finished product.
[0019] Using the fabric softener provided in this embodiment to treat repeatedly wash...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com