Embodiment 1
[0016] Put the lithopone into a grinder and grind until the particle size is less than 50 microns, transfer 2.5 kg of water, 0.2 kg of paraffin, 0.15 kg of glycerol and 0.4 kg of ground lithopone into a high-speed disperser, and grind at 1800 rpm Disperse for 50 minutes under the speed of rotation; transfer the obtained material to the mixer, add 0.5 kg of nano silicon dioxide, 0.7 kg of silicon acrylic emulsion and 4 kg of film-forming material in turn while stirring, control the stirring speed to 550 rpm, and mix well Detect the viscosity of the solution, when the viscosity of the mixed solution is 96KU, filter to obtain the scrub-resistant wall paint.
Embodiment 2
[0018] Put the lithopone into a grinder and grind until the particle size is less than 50 microns, transfer 30 kg of water, 2.5 kg of paraffin, 2 kg of glycerin and 3 kg of ground lithopone into a high-speed disperser, at 1500 rpm Disperse for 45 minutes under the speed of rotation; transfer the resulting material to the mixer, add 4 kg of nano-silica, 5 kg of silicon-acrylic emulsion and 30 kg of film-forming material successively while stirring, control the stirring speed to 600 rpm, and mix evenly Detect the viscosity of the solution, when the viscosity of the mixed solution is 93KU, filter to obtain the scrub-resistant wall paint.
Embodiment 3
[0020] Put the lithopone into a grinding machine and grind until the particle size is less than 50 microns, transfer 200 kg of water, 22.5 kg of paraffin, 10 kg of glycerol and 50 kg of ground lithopone into a high-speed disperser, at 1500 rpm Disperse for 60 minutes under the speed of rotation; transfer the obtained material to the mixer, add 30 kg of nano silicon dioxide, 60 kg of silicon acrylic emulsion and 350 kg of film-forming material in turn while stirring, control the stirring speed to 500 rpm, and mix well Detect the viscosity of the solution, when the viscosity of the mixed solution is 100KU, filter to obtain the scrub-resistant wall paint.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com