A kind of processing method of antique wood
A processing method and technology for wood, applied in wood processing, wood processing details, wood heating and other directions, can solve the problems of complicated methods, a large number of chemical preparations, and high processing costs, and achieve less damage to wood structure, simple process, and good anti-corrosion performance. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A processing method for antique wood, comprising the following steps:
[0017] (1) To prepare slurry treatment, take 45 parts of dried river bottom sludge, 3 parts of iron oxide, 7 parts of sodium hexametaphosphate, 0.8 parts of potassium permanganate, and 70 parts of water, mix them, and stir for 45 minutes at a speed of 85 r / min , make it fully mixed to get the treated slurry;
[0018] (2) Wood surface treatment: Clean the wood surface to remove debris and dust on the wood surface, and then apply the treatment slurry prepared in step (1) evenly on the wood surface, and the thickness of the treatment slurry is 3cm;
[0019] (3) Baking, the wood treated in step (2) is baked in an oven, the temperature in the oven is controlled at 75°C, and the baking time is 4 hours;
[0020] (4) Paint, after the wood is baked, remove the mud on the surface of the wood, use sandpaper to polish the outer surface of the wood, fill it with putty after polishing, and then spray paint;
[...
Embodiment 2
[0023] A processing method for antique wood, comprising the following steps:
[0024] (1) To prepare slurry treatment, take 48 parts of dried river bottom sludge, 5 parts of iron oxide, 6 parts of sodium hexametaphosphate, 1 part of potassium permanganate, and 80 parts of water, mix them, and stir at 90r / min for 35min , making it fully mixed to obtain the treated slurry;
[0025] (2) Wood surface treatment: Clean the wood surface to remove debris and dust on the wood surface, and then apply the treatment slurry prepared in step (1) evenly on the wood surface, and the thickness of the treatment slurry is 4cm;
[0026] (3) Baking, the wood treated in step (2) is baked in an oven, the temperature in the oven is controlled at 75°C, and the baking time is 5 hours;
[0027] (4) Paint, after the wood is baked, remove the mud on the surface of the wood, use sandpaper to polish the outer surface of the wood, fill it with putty after polishing, and then spray paint;
[0028] (5) For s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com