[0008] Embodiment 1 A paint is characterized in that it is made of the following raw materials in parts by mass: 30 parts of paint, 6 parts of zeolite powder, 5 parts of natural jade powder, 11 parts of rosin resin and linseed oil mixture, 6 parts of hydroxyethyl cellulose 6 parts, water-based acrylic acid 6 parts.
[0009] Described paint preparation process is as follows:
[0010] 1) Put the paint, zeolite powder, natural jade powder and water-based acrylic acid into the processing equipment according to the amount of each content, control the temperature at 45°C-75°C, and then stir for 10-15 minutes to make it uniform Thin paint; 2) Then add hydroxyethyl cellulose and a mixture of rosin resin and linseed oil with coagulation effect to the diluted paint, stir evenly for 15 minutes, and process the finished paint in the equipment; 3) Finally, the paint is passed through a special The equipment is installed in the paint canister.
Embodiment 2
[0012] A paint, characterized in that it is made from the following raw materials in parts by mass: 50 parts of paint, 9 parts of zeolite powder, 10 parts of natural jade powder, 15 parts of rosin resin and linseed oil mixture, 10 parts of hydroxyethyl cellulose, water-based Acrylic 10 parts.
[0013] Described paint preparation process is as follows:
[0014] 1) Put the paint, zeolite powder, natural jade powder and water-based acrylic acid into the processing equipment according to the amount of each content, control the temperature at 45°C-75°C, and then stir for 10-15 minutes to make it evenly Thin paint; 2) Then add hydroxyethyl cellulose and a mixture of rosin resin and linseed oil with coagulation effect to the diluted paint, stir evenly for 15 minutes, and process the finished paint in the equipment; 3) Finally, the paint is passed through a special The equipment is installed in the paint canister.
Embodiment 3
[0016] A paint, characterized in that it is made of the following raw materials in parts by mass: 40 parts of paint, 8 parts of zeolite powder, 8 parts of natural jade powder, 12 parts of rosin resin and linseed oil mixture, 8 parts of hydroxyethyl cellulose, water-based Acrylic 8 parts.
[0017] Described paint preparation process is as follows:
[0018] 1) Put the paint, zeolite powder, natural jade powder and water-based acrylic acid into the processing equipment according to the amount of each content, control the temperature at 45°C-75°C, and then stir for 10-15 minutes to make it uniform Thin paint; 2) Then add hydroxyethyl cellulose and a mixture of rosin resin and linseed oil with coagulation effect to the diluted paint, stir evenly for 15 minutes, and process the finished paint in the equipment; 3) Finally, the paint is passed through a special The equipment is installed in the paint canister.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com