A production method and concrete technology, which is applied in the manufacture of tools, ceramic molding machines, etc., can solve the problems of time-consuming and labor-intensive production, long natural curing time of concrete, and long production cycle, so as to improve the anti-seismic cracking performance and penetration ability , the effect of improving the overall strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] A method for making an anti-seismic crack-proof concrete square pile:
[0028] 1. Design the concrete mixing ratio. 125 parts of gravel, 350 parts of yellow sand, 98 parts of water reducing agent, 210 parts of cement, 34 parts of anti-seismic mixture and 20 parts of anti-cracking polymer fiber mixture. Concrete preparation: Add in sequence according to the designed concrete mixing ratio, add water and mix evenly, and stir for 100s.
[0029] The weight components of each raw material when preparing the anti-seismic mixture are: 16 parts of industrial aluminum sulfate, 1 part of sodium lauryl sulfate, 18 parts of silica fume, 20 parts of anhydrite, 14 parts of sulfoaluminate cooked material.
[0030] The anti-cracking polymer fiber mixture is used to prepare the raw material components and its parts by weight are 70 parts of polyacryl alcohol fiber and 30 parts of polybutene fiber.
[0031] 2. Pouring. Including mold opening artificial fabric, mold clamping pump mater...
Embodiment 2
[0038] On the basis of Example 1, the design concrete mixing ratio was changed: specifically, 135 parts of gravel, 480 parts of yellow sand, 102 parts of water reducing agent, 250 parts of cement, 45 parts of anti-seismic mixture and 80 parts of anti-cracking polymer fiber mixture. Concrete preparation: Add in sequence according to the designed concrete mixing ratio, add water and mix evenly, and stir for 100s.
[0039] The weight components of each raw material when preparing the anti-seismic mixture are: 26 parts of industrial aluminum sulfate, 5 parts of sodium lauryl sulfate, 35 parts of silica fume, 38 parts of anhydrite, 25 parts of sulphoaluminate cooked material.
[0040] The anti-cracking polymer fiber mixture is used to prepare the raw material components and its parts by weight are 80 parts of polyacryl alcohol fiber and 20 parts of polybutene fiber.
[0041] Carry out the finished product according to the preparation method of embodiment 1.
[0042] The anti-seis...