A nano-composite material and polymer-based technology, which is applied in the field of polymer-based nano-composite materials for earphone wires and its preparation, can solve the problems of breaking the balance state, losing the unique functions and effects of nanoparticles, and improving water resistance and nano-characteristics. Maintain good and improve the effect of comprehensive performance

Active Publication Date: 2018-01-23
DONGGUAN YINGTONG WIRE +1
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] Existing polymer-based nanocomposites and their preparation methods often have extremely high surface energy and a strong tendency to agglomerate due to the high surface energy of inorganic nanoparticles. It is originally a dispersed equilibrium state, and what is often obtained is that the nanoparticles are agglomerated into composite materials with a scale of hundreds of nanometers or even micrometers, thus losing the unique functions and effects of nanoparticles.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] Example 1 The polymer-based nanocomposite material for earphone wire provided in this example is made of the following components in parts by weight: 20-30 parts of water-based polyurethane nanocomposite emulsion, 30-40 parts of oil plasticizer, 6-10 parts of sodium stearate, 10-20 parts of calcium carbonate.

[0028] Further, the oil plasticizer is any one or both of paraffin oil, white oil and naphthenic oil.

[0029] Further, the components and mass ratios contained in the water-based polyurethane nanocomposite emulsion are organically modified medical stone dispersion 0.05: polymer diol 2.8: HDI trimer 1.2: water-soluble chitosan 2.3: Catalyst Dibutyltin dilaurate 0.03: Trimethylolpropane 0.3: Antioxidant 1010 0.015: Triethylamine 0.2: Deionized water 10: Ethylenediamine 0.04.

[0030] Further, the polymer diol is one or both of polytetrahydrofuran ether diol, polypropylene glycol and polycaprolactone diol, and the molecular weight of the polymer diol is 1000-4000;...

Embodiment 2

[0044] The polymer-based nanocomposite material for earphone wire provided in this embodiment and its preparation method are basically the same as those in Embodiment 1, except that:

[0045] A polymer-based nanocomposite material for earphone wires, which is made of the following components in parts by weight: 20 parts of water-based polyurethane nanocomposite emulsion, 40 parts of paraffin oil, 10 parts of sodium stearate, and 10 parts of calcium carbonate.

[0046] Further, the components and mass ratios contained in the water-based polyurethane nanocomposite emulsion are organically modified medical stone dispersion 0.05: polytetrahydrofuran ether glycol 2.8: HDI trimer 1.2: water-soluble chitosan 2.3: Catalyst Dibutyltin dilaurate 0.03: Trimethylolpropane 0.3: Antioxidant 1010 0.015: Triethylamine 0.2: Deionized water 10: Ethylenediamine 0.04. Wherein, the concentration of the organically modified medical stone dispersion is 1mg / ml, and the raw material components and wei...

Embodiment 3

[0055] The polymer-based nanocomposite material for earphone wire provided in this embodiment and its preparation method are basically the same as those in Embodiments 1 and 2, except that:

[0056] A polymer-based nanocomposite material for earphone wires, which is made of the following components in parts by weight: 25 parts of aqueous polyurethane nanocomposite emulsion, 40 parts of white oil, 8 parts of sodium stearate, and 20 parts of calcium carbonate.

[0057] Further, the components and mass ratios contained in the water-based polyurethane nanocomposite emulsion are organically modified medical stone dispersion 0.05: polypropylene glycol 2.8: HDI trimer 1.2: water-soluble chitosan 2.3: catalyst dilaurel Dibutyltin acid 0.03: Trimethylolpropane 0.3: Antioxidant 1010 0.015: Triethylamine 0.2: Deionized water 10: Ethylenediamine 0.04. Wherein, the concentration of the organically modified medical stone dispersion is 2mg / ml, and the raw material components and weight perce...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
particle diameteraaaaaaaaaa
concentrationaaaaaaaaaa
concentrationaaaaaaaaaa
Login to view more

Abstract

The invention discloses a polymer-based nano-composite material for earphone wires, which is made of the following components in parts by weight: 20-30 parts of water-based polyurethane nano-composite emulsion, 30-40 parts of oil plasticizer, hard 6-10 parts of sodium bicarbonate, 10-20 parts of calcium carbonate; Wherein, the component and the mass ratio contained in the described aqueous polyurethane nanocomposite emulsion are organically modified medical stone dispersion 0.05: polymer glycol 2.8 : HDI trimer 1.2: Water-soluble chitosan 2.3: Catalyst dibutyltin dilaurate 0.03: Trimethylolpropane 0.3: Antioxidant 10100.015: Triethylamine 0.2: Deionized water 10: Ethylenediamine 0.04. The invention also discloses a preparation method of the polymer-based nanocomposite material for the earphone wire. The invention uses organically modified medical stone and chitosan to modify the water-based polyurethane, which has the properties of water resistance, aging resistance, yellowing resistance, stain resistance, abrasion resistance, antibacterial and radiation resistance, and is suitable for Applied to the outer coating material of the earphone wire to improve the overall performance.

Description

technical field [0001] The invention relates to the field of nanocomposite materials, in particular to a polymer-based nanocomposite material for earphone wires and a preparation method thereof. Background technique [0002] The polymer-based composite material not only maintains various excellent properties of the polymer matrix itself, but also can give full play to the specific performance of the nano-units, and can also inhibit the oxidation and aggregation of the nano-units, so that the system has high long-term stability. Nano-modified waterborne polyurethane materials overcome the defects of waterborne polyurethane water resistance and weather resistance, improve the material's water resistance, aging resistance, stain resistance, thermal stability and wear resistance, and can also make waterborne polyurethane antibacterial and radiation resistant , deodorant and other properties. [0003] Medical stone is a compound mineral or medicinal rock that is non-toxic and ha...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): C08L75/04C08L91/06C08L5/08C08K13/06C08K9/06C08K3/34C08K3/32C08K5/098C08K3/26C08K5/01C08G18/79C08G18/66C08G18/64
Inventor 傅华良李海龙
Owner DONGGUAN YINGTONG WIRE
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products