[0012] Embodiment 1: raw material and consumption of preparing environmental protection shopping bag:
[0013] 15 kg of linear low-density polyethylene, 15 kg of ground calcium carbonate powder, 3 kg of ethylene-butylene copolymer, 18 kg of a blend of starch and polyvinyl alcohol, 15 kg of polyethylene, and 0.1 kg of toner.
[0014] The preparation method is as follows: add heavy calcium carbonate powder into a high-speed mixer, seal, heat and stir, the heating temperature is 70°C-80°C, and the stirring time is 3 minutes, open the sealing cover to disperse the mist, and then add polyethylene and linear low-density polyethylene , continue heating and stirring, the heating temperature is 70°C to 80°C, stir for 10 minutes, add ethylene butene copolymer and toner to obtain a mixed material; then the blend of starch and polyvinyl alcohol is extruded from the twin-screw extruder Add the fiber adding port, put the mixture obtained above into the twin-screw extruder, heat it to 190°C-...
Embodiment 2
[0015] Embodiment 2: prepare the raw material of environmental protection shopping bag and consumption:
[0016] 18 kg of linear low-density polyethylene, 25 kg of ground calcium carbonate powder, 2 kg of ethylene-butylene copolymer, 15 kg of a blend of starch and polyvinyl alcohol, 18 kg of polyethylene, and 1 kg of toner.
[0017] The preparation method is as follows: add heavy calcium carbonate powder into a high-speed mixer, seal, heat and stir, the heating temperature is 70°C-80°C, the stirring time is 5 minutes, open the sealing cover to disperse the mist, and then add polyethylene and linear low-density polyethylene , continue heating and stirring, the heating temperature is 70°C to 80°C, stir for 10 minutes, add ethylene butene copolymer and toner to obtain a mixed material; then the blend of starch and polyvinyl alcohol is extruded from the twin-screw extruder Add the fiber adding port, put the mixture obtained above into the twin-screw extruder, heat it to 190°C-210°...