Lightweight high strength material for tunnel and underground pipeline construction and preparation method of lightweight high strength material
An underground pipeline and lightweight technology, applied in the field of lightweight and high-strength materials and their preparation, can solve the problem of high cost of steel-concrete structures, and achieve the effects of excellent corrosion resistance, simple preparation and easy operation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] The preparation of the above-mentioned lightweight and high-strength materials for tunnel or underground pipeline construction includes the following steps:
[0017] Step 1. Preparation of preservatives: Weigh each component and mix them evenly in a mixer, transfer to a grinder and grind to a predetermined fineness, and vacuum-seal packaging;
[0018] Step 2. Preparation of lightweight high-strength material: Weigh each component and mix evenly, add water and stir for 2 minutes, and mix evenly.
Embodiment 2
[0020] The preparation of the above-mentioned lightweight and high-strength materials for tunnel or underground pipeline construction includes the following steps:
[0021] Step 1. Preparation of preservatives: Weigh each component and mix them evenly in a mixer, transfer to a grinder and grind to a predetermined fineness, and vacuum-seal packaging;
[0022] Step 2. Preparation of lightweight high-strength material: Weigh each component and mix evenly, add water and stir for 5 minutes, and mix evenly.
Embodiment 3
[0024] The preparation of the above-mentioned lightweight and high-strength materials for tunnel or underground pipeline construction includes the following steps:
[0025] Step 1. Preparation of preservatives: Weigh each component and mix them evenly in a mixer, transfer to a grinder and grind to a predetermined fineness, and vacuum-seal packaging;
[0026] Step 2. Preparation of lightweight high-strength material: Weigh each component and mix evenly, add water and stir for 3 minutes, and mix evenly.