A solvent-free, synthetic leather technology, applied in the field of synthetic leather manufacturing, can solve problems such as being unfavorable to health and environmental protection, and achieve the effects of strong skin and skin feel, advanced preparation technology, and zero-solvent use, health and environmental protection
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0050] The synthetic leather of this embodiment includes a water-based surface layer and a solvent-free middle layer. Foaming polyurethane resin, the two-component material is a polyether type combination A material and a polyether type B material prepolymer.
[0051] In this embodiment, the preparation method of water-based / solvent-free composite environmentally friendly polyurethane synthetic leather specifically includes the following steps:
[0052] (1) Preparation of the water-based surface layer: Coat the water-based surface layer slurry on the release paper, control the coating thickness of the water-based surface layer slurry to 0.2mm, dry at 120°C for 3 minutes, and then solidify and form to obtain the water-based surface layer;
[0053] The water-based surface layer is a thermosetting polyether water-based polyurethane resin;
[0054] The proportioning of each raw material by mass parts in the water-based surface layer slurry is:
[0055]
[0056] (2) Preparation ...
Embodiment 2
[0062] The synthetic leather of this embodiment includes a water-based surface layer and a solvent-free middle layer. Foaming polyurethane resin, the two-component material is a polyether type combination A material and a polyether type B material prepolymer.
[0063] In this embodiment, the preparation method of water-based / solvent-free composite environmentally friendly polyurethane synthetic leather specifically includes the following steps:
[0064] (1) Preparation of the water-based surface layer: Coat the water-based surface layer slurry on the release paper, control the coating thickness of the water-based surface layer slurry to 0.4mm, dry at 130°C for 3 minutes, and then solidify and form to obtain the water-based surface layer;
[0065] The water-based surface layer is a thermosetting polyether water-based polyurethane resin;
[0066] The proportioning of each raw material by mass parts in the water-based surface layer slurry is:
[0067]
[0068] (2) Preparatio...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com