[0040] (1) Take 1 gram of sodium alginate polymer, 1 gram of carrageenan, 0.03 gram of xanthan gum, 0.1 gram of hydroxymethylcellulose, 2 grams of propylene glycol, and 2 grams of glycerin and mix them uniformly to make a mixture;
[0041] (2) Add 93.82 grams of deionized water to the mixture in step (1) according to the mass ratio, and stir again to form a liquid mixture;
[0042] (3) Put the liquid mixture in step (2) into an emulsifier that has been preheated to 50°C and heat and stir for 30 minutes to make an emulsion;
[0043] (4) Add 0.05 gram of Cathone to step (3) emulsion, and stir evenly, make finished product liquid;
[0044] (5) heat and defoam the finished product liquid in step (4) for 5min;
[0045] (6) Discharging and filling the finished liquid in step (5) to make a circular patch of MP-A type circular specification, diameter×thickness 90×8mm.
Embodiment 2
[0047] (1) Get 3 grams of sodium alginate polymer, 2.5 grams of carrageenan, 0.04 grams of xanthan gum, 0.4 grams of hydroxymethylcellulose, 7.5 grams of propylene glycol, and 7.5 grams of glycerin and mix them uniformly to make a mixture;
[0048] (2) Add 79 grams of deionized water to the mixture in step (1) according to the mass ratio, and stir again to form a liquid mixture;
[0049] (3) Put the liquid mixture in step (2) into an emulsifier that has been preheated to 75°C and heat and stir for 30 minutes to make an emulsion;
[0050] (4) Add 0.06 gram of Cathone to step (3) emulsion, and stir evenly, make finished product liquid;
[0051] (5) Insulating and defoaming the finished product liquid in step (4) for 15min;
[0052] (6) Discharging and filling the finished liquid in step (5) to make a B1 patch of irregular specification MP-B type.
Embodiment 3
[0054] (1) Get 6 grams of sodium alginate polymer, 5 grams of carrageenan, 0.05 grams of xanthan gum, 0.8 grams of hydroxymethylcellulose, 15 grams of propylene glycol, and 15 grams of glycerin and mix them uniformly to make a mixture;
[0055] (2) Add 58.03 grams of deionized water to the mixture in step (1) according to the mass ratio, and stir again to form a liquid mixture;
[0056] (3) Put the liquid mixture in step (2) into an emulsifier that has been preheated to 100°C and heat and stir for 30 minutes to make an emulsion;
[0057] (4) Add the mixture of 0.12 gram methyl ester and propyl ester to step (3) emulsion, and stir, make finished product liquid;
[0058] (5) Insulating and defoaming the finished product liquid in step (4) for 30min;
[0059] (6) Discharging and filling the finished liquid in step (5) to make it into a circular specification for ultrasonic focus therapy equipment, diameter×thickness: 200×4mm.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com