An electric heater that generates biological waves after electrification and its manufacturing method
A manufacturing method and technology of electric heating sheet, which are applied in the direction of coating, metal material coating process, melting spray plating, etc., can solve the problems of insufficient use effect and convenience of physical health care equipment, unsafe food, and large side effects. Effects of blood circulation and metabolism, final density increase, pH balance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] A method for manufacturing a heating element that generates biological waves after electrification, comprising the following steps:
[0027] Step 1) Proportioning according to the following ingredients in percentage by weight: tourmaline powder 8%; silicon powder 60%; iron powder 8%; copper powder 4%; silicon carbide 4%; graphite powder 6%; molybdenum disilicide powder 4% ; Aluminum oxide 1%; Titanium dioxide 0.4%; Magnesium oxide 0.6%; Dextrin binder 4%, the particle size of each of the above powders is above 200 mesh;
[0028] Step 2) Mixing: Stir and mix the above raw materials;
[0029] Step 3) Grinding and forming: Pour the mixture in step 2) into a mold and use a press to form it. The length of the mold is 200mm, the width is 20mm, and the thickness is 5mm. The tonnage of the press is 60T- 100T;
[0030] Step 4) demoulding and air-drying: demoulding the pressed mixture to obtain a core material, and placing the core material on a plane for natural air-drying;
...
Embodiment 2
[0034] It differs from Example 1 in that: tourmaline powder 9%; silicon powder 57.8%; iron powder 8%; copper powder 4%; silicon carbide 4%; graphite powder 7%; molybdenum disilicide powder 4%; aluminum oxide 1.2% ; titanium dioxide 0.4%; magnesium oxide 0.6%;
Embodiment 3
[0036] It differs from Example 1 in that: tourmaline powder 9%; silicon powder 57.5%; iron powder 8%; copper powder 4%; silicon carbide 4%; graphite powder 7%; molybdenum disilicide powder 4%; aluminum oxide 1.3% ; titanium dioxide 0.4%; magnesium oxide 0.8%; dextrin binder 4%, the heating period is 14h, the temperature of the holding period is kept at 1400 ℃, and the cooling period is 14h.
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size (mesh) | aaaaa | aaaaa |
| length | aaaaa | aaaaa |
| width | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com