A technology for discarding refractory materials and metallic copper, which is applied in the directions of flotation, process efficiency improvement, solid separation, etc., can solve problems such as environmental pollution, achieve the effect of improving copper grade, inhibiting gangue magnesia, and avoiding large consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Example Embodiment
[0036] Example 1:
[0037] The waste refractory bricks of a copper converter in Guangdong are used as raw materials, and the copper content of the refractory bricks is 5.48%. The sample is first crushed-ball-milled until 86% of the samples are smaller than 0.074mm, and then the ground slurry is poured into the flotation cell for flotation test; a. One flotation: the sample poured into the flotation cell is slurried , After fully stirring, add 200g / t kerosene as an auxiliary collector and stir for 8 minutes, then add 400g / t xanthate as a collector and stir for 4 minutes, and then add 50g / t as a foaming agent. After terpineol, stir for 2 minutes, flotation for 4 minutes to obtain primary flotation concentrate and primary flotation tailings; b. Secondary flotation: continue to add 200g / t of pentoxanthate to the primary flotation tailings and stir for 4 minutes, Then add 30g / t terpineol as a foaming agent, stir for 2 minutes, flotation for 4 minutes to obtain secondary flotation ...
Example Embodiment
[0039] Example 2:
[0040]The waste magnesia-chromium refractory bricks of a copper converter in Hubei are used as raw materials, and the copper content of the refractory bricks is 4.82%. The sample is first crushed-ball-milled until 82% of the sample is smaller than 0.074mm, and then the ground slurry is poured into the flotation cell for flotation test; a. One flotation: the sample poured into the flotation cell is slurried , After fully stirring, add 300g / t sodium sulfide as a vulcanizing agent and stir for 8 minutes, then add 200g / t kerosene as an auxiliary collector and stir for 8 minutes, and then add 400g / t pentoxide as a collector. After stirring for 4 minutes, finally adding 60g / t terpineol as a foaming agent, stirring for 2 minutes, and flotation for 5 minutes to obtain primary flotation concentrate and primary flotation tailings; b. Secondary flotation: after primary flotation Continue to add 150g / t of sodium sulfide as a vulcanizing agent to the tailings and stir ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap