An optical information code and information recording technology, applied in the field of optical information code reading, can solve the problems of low reading accuracy, the QR code scanner cannot determine the two-dimensional code image, the barcode image cannot be determined, etc., to improve reading The effect of accuracy
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0195]
[0196] A thermoreversible recording medium that reversibly changes color tone by the action of heat is produced as follows.
[0197] -Support-
[0198] A white polyester film (TETRON (registered trademark) film U2L98W, manufactured by Teijin Dupont Co.) having an average thickness of 125 μm was prepared as the support.
[0199] -Formation of the first oxygen barrier layer-
[0200] Polyurethane adhesive (TM-567, manufactured by Toyo-Morton, Ltd.) (5 parts by mass), isocyanate (CAT-RT-37, manufactured by Toyo-Morton, Ltd.) (0.5 parts by mass), and ethyl acetate (5 parts by mass) were mixed together, followed by stirring sufficiently to prepare an oxygen barrier layer coating liquid.
[0201] Then, the prepared coating liquid for oxygen barrier layer was applied to a silica-evaporated PET film (TECHBARRIER HX, oxygen permeability: 0.5 mL / m 2 / day / MPa, manufactured by Mitsubishi Plastics Inc.), followed by heating and drying at 80° C. for 1 minute. This silica-evap...
Embodiment 2
[0222]
[0223] The thermoreversible recording medium of Production Example 2 was produced in the same manner as Production Example 1 except that the second oxygen barrier layer was not formed.
Embodiment 3
[0225]
[0226] A thermoreversible recording medium in which the color tone of the thermoreversible recording medium is reversibly changed is produced.
[0227] -Support-
[0228] As the support, a white polyester film (Tetron (registered trademark) film U2L98W, manufactured by Teijin DuPont Films Japan Limited) having an average thickness of 125 μm was provided.
[0229] -Thermosensitive recording layer-
[0230] By means of a ball mill, 6 parts by mass of octadecylphosphonic acid as a developer, 16 parts by mass of 10% by mass polyvinyl alcohol acetoacetal (plyvinyl acetoacetal) solution (KS-1, produced by Sekisui Chemical Co., Ltd. .manufacturing), 12 parts by mass of toluene, and 3 parts by mass of methyl ethyl ketone were ground and dispersed until their average particle diameter was about 0.3 μm. To the resulting dispersion, 1.5 parts by mass of 2-aniline-3-methyl-6-diethylaminofluorene as a leuco dye, and 0.37 parts by mass of 1.85% by mass of LaB 6 A dispersion li...