Embodiment 1
[0025] The sizing process of wool fabric yarn comprises the steps:
[0026] 1) Put 1-2 parts by weight of mineral oil, 1.5 parts by weight of modified silicone oil, 1.4 parts by weight of styrene, 0.7 parts by weight of gum arabic powder, and 12 parts by weight of alginate into 30 parts by weight of deionized water in sequence, and stir evenly;
[0027] 2) drop into 1.1 parts by weight of coconut oil fatty acid diethanolamide, 0.8 parts by weight of sodium alkylnaphthalene sulfonate, 2.1 parts by weight of diethylene glycol monobutyl ether, 0.8 parts by weight of tert-butylhydroquinone, and continue to stir, Until fully mixed evenly, a slurry is obtained;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 2
[0030] The sizing process of wool fabric yarn comprises the steps:
[0031] 1) Put 1 part by weight of mineral oil, 1.5 parts by weight of modified silicone oil, 1.4 parts by weight of styrene, 0.7 parts by weight of gum arabic powder, and 12 parts by weight of alginate into 30 parts by weight of deionized water, and stir evenly;
[0032] 2) drop into 1.1 parts by weight of coconut oil fatty acid diethanolamide, 0.8 parts by weight of sodium alkylnaphthalene sulfonate, 2.1 parts by weight of diethylene glycol monobutyl ether, 0.8 parts by weight of tert-butylhydroquinone, and continue to stir, Until fully mixed evenly, a slurry is obtained;
[0033] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 3
[0035] The sizing process of wool fabric yarn comprises the steps:
[0036] 1) Put 2 parts by weight of mineral oil, 1.5 parts by weight of modified silicone oil, 1.4 parts by weight of styrene, 0.7 parts by weight of gum arabic powder, and 12 parts by weight of alginate into 30 parts by weight of deionized water, and stir evenly;
[0037] 2) drop into 1.1 parts by weight of coconut oil fatty acid diethanolamide, 0.8 parts by weight of sodium alkylnaphthalene sulfonate, 2.1 parts by weight of diethylene glycol monobutyl ether, 0.8 parts by weight of tert-butylhydroquinone, and continue to stir, Until fully mixed evenly, a slurry is obtained;
[0038] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com