Wool fabric yarn sizing process
A yarn and fabric technology, which is applied in the field of sizing process of wool fabric yarn, can solve the problems that the performance needs to be improved, and achieve the effects of increased strength, yarn hairiness fit, and good elongation performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The sizing process of wool fabric yarn comprises the steps:
[0026] 1) Put 1 to 2 parts by weight of water-soluble polyacrylic acid, 1.2 parts by weight of sodium chloride, 1.6 parts by weight of polyurethane resin, 1.4 parts by weight of hydroxypropyl cellulose, and 12 parts by weight of polyvinyl alcohol into 20 parts by weight of deionized water , stir evenly;
[0027] 2) Add 1.3 parts by weight of distearyldimethylammonium chloride, 0.6 parts by weight of lauryl betaine, 1.6 parts by weight of polyvinyl alcohol, and 1.3 parts by weight of polyether ester amide in turn, and continue stirring until fully mixed Homogenously, make a slurry;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 2
[0030] The sizing process of wool fabric yarn comprises the steps:
[0031] 1) 1 part by weight of water-soluble polyacrylic acid, 1.2 parts by weight of sodium chloride, 1.6 parts by weight of polyurethane resin, 1.4 parts by weight of hydroxypropyl cellulose, and 12 parts by weight of polyvinyl alcohol are dropped into 20 parts by weight of deionized water in sequence, and stirred Uniform;
[0032] 2) Add 1.3 parts by weight of distearyldimethylammonium chloride, 0.6 parts by weight of lauryl betaine, 1.6 parts by weight of polyvinyl alcohol, and 1.3 parts by weight of polyether ester amide in turn, and continue stirring until fully mixed Homogenously, make a slurry;
[0033] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 3
[0035] The sizing process of wool fabric yarn comprises the steps:
[0036] 1) Put 2 parts by weight of water-soluble polyacrylic acid, 1.2 parts by weight of sodium chloride, 1.6 parts by weight of polyurethane resin, 1.4 parts by weight of hydroxypropyl cellulose, and 12 parts by weight of polyvinyl alcohol into 20 parts by weight of deionized water in turn, and stir Uniform;
[0037] 2) Add 1.3 parts by weight of distearyldimethylammonium chloride, 0.6 parts by weight of lauryl betaine, 1.6 parts by weight of polyvinyl alcohol, and 1.3 parts by weight of polyether ester amide in turn, and continue stirring until fully mixed Homogenously, make a slurry;
[0038] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com