Composite dressing applied to wound and preparation method thereof
A wound and compound technology, applied in the fields of application, chemical instruments and methods, and pharmaceutical formulations, can solve problems such as pain, re-cracking, and easily involved wounds, and achieve the effects of accelerating wound healing, promoting regeneration, and having no toxic side effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0049] A composite dressing applied to wounds. The dressing is composed of hair keratin and traditional Chinese medicine ingredients. The traditional Chinese medicine ingredients include Panax notoginseng, Chonglou, Dustin, borneol and musk.
[0050] The weight ratio of hair keratin and Chinese medicine components is 1-3:3-1, preferably 1:1-2, for example 1:1.
[0051] The parts by weight of the various ingredients in the Chinese medicine ingredients can be: ① 20 parts of Panax notoginseng, 25 parts of Chonglou, 10 parts of Dingzi, 20 parts of Borneolum and 0.001 part of musk; ② 40 parts of Panax notoginseng, 10 parts of Chonglou, 20 parts of stator, 40 parts of borneol and 0.8 part of musk; ③ 30 parts of Sanqi, 18 parts of Chonglou, 15 parts of independent stator, 30 parts of borneol and 0.1 part of musk; ④ 25 parts of Panax notoginseng, 12 parts of Chonglou, 18 of independent stator 35 parts of borneol and 0.03 part of musk; ⑤ 33 parts of Panax notoginseng, 23 parts of Chong...
Embodiment 2
[0056] A kind of preparation method of the compound type dressing that root is applied to wound surface, the concrete method of this method is as follows:
[0057] (1) Preparation of hair keratin:
[0058] S1: Degreasing: Weigh 5g of hair and put it in a 1000ml beaker. Add 99.7% absolute ethanol to soak for 30 minutes, stir once with a glass rod every 5 minutes, and rinse with running water;
[0059] S2: Softening: Place the washed hair in a solution of ≥10% sodium hypochlorite 10ml and distilled water 90ml, soak at room temperature for 30 minutes, stir with a glass rod once every 5 minutes, and rinse with running water;
[0060] S3: decolorization: by the weight of 5g hair, take by weighing 99% sodium pyrophosphate (Na 4 P 2 o 7 )4g, 99.5% potassium persulfate (K 2 S 2 o 8 ) 1.5g, 30% hydrogen peroxide (H 2 o 2 ) 80ml, 25% concentrated ammonia water 27.5ml, distilled water 400ml, make a decolorization solution, put the softened hair in this solution, put it in a cons...
Embodiment 3
[0076] The gelling among the present invention gets the preparation method of hair keratin and can be any one of following two kinds of methods:
[0077] 1. Weigh the high-purity granular hair keratin 50mg obtained in the present invention (for example, Example 2) and add 5ml of water, mix thoroughly, place in an incubator and incubate for 2-3 hours until a relatively uniform Color and character; Sterilize, obtain gelled hair keratin, its concentration is 1%.
[0078] 2. S1: Weigh 10g of wool or human hair, put it into a three-neck flask containing a mixed solution of 180ml of absolute ethanol and 20ml of distilled water, heat it for 15 minutes and then raise the temperature to 75°C, and the solution starts to reflux; then, drip while refluxing Add 2ml of NaOH solution until the pH value of the oxidized keratin is 7, the reflux and dropwise addition are completed at the same time, and the time lasts for 90 minutes; after the dropwise addition and reflux are completed, continue...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com