Copper-molybdenum separation electric potential flotation process
A potential and flotation technology, applied in flotation, solid separation, etc., can solve the problems of difficult control of foam grade, high production cost, and influence on molybdenum recovery rate, so as to stabilize foam grade, increase recovery rate, and inhibit copper minerals Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] Copper-molybdenum separation potential flotation process, including raw ore crushing, ore grinding steps, mixed flotation steps, and separation flotation steps. In the separation flotation step, the pH value of the ore pulp is kept at 10, and the concentration of copper and molybdenum separation is set. At 42%, the flow rate is set at 45 m3 / h, and the potential of the roughing pulp is controlled at -530mv by adding the amount of sodium hydrosulfide. Then, 180ml / min of polyacrylamide modified substance is added as a copper inhibitor to separate the rough The selected molybdenum foam grade is controlled at 9-12%, and the copper grade is controlled at 11.2-15%. The grade ranges of copper and molybdenum for other operations are: Refined 1: Molybdenum 10.5-14.5%, containing 10-13% copper; Refined 2: Molybdenum 16.7-20.3%, containing copper 9.8-12.4%; Refined 3: Molybdenum 20.1- 26.0%, containing 7.3-10.4% copper; refined four: molybdenum 24.7-32.0%, containing 5.3-7.6% coppe...
Embodiment 2
[0010] Copper-molybdenum separation potential flotation process, including raw ore crushing, ore grinding steps, mixed flotation steps, and separation flotation steps. In the separation flotation step, the pH value of the ore pulp is kept at 11, and the concentration of copper and molybdenum separation is set. At 40%, the flow rate is set at 40 m3 / h, and the potential of the roughing pulp is controlled at -510mv by adding the amount of sodium hydrosulfide. Then, 180ml / min of polyacrylamide modified substance is added as a copper inhibitor to separate the coarse The selected molybdenum foam grade is controlled at 9-12%, and the copper grade is controlled at 11.2-15%. The grade ranges of copper and molybdenum for other operations are: Refined 1: Molybdenum 10.5-14.5%, containing 10-13% copper; Refined 2: Molybdenum 16.7-20.3%, containing copper 9.8-12.4%; Refined 3: Molybdenum 20.1- 26.0%, containing 7.3-10.4% copper; refined four: molybdenum 24.7-32.0%, containing 5.3-7.6% copp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com