A repairing material and temperature repairing technology, which is applied in the field of pavement pothole repairing materials, can solve problems such as unsatisfactory technical performance and durability, uneven heating of the road surface, increased material costs, etc., and achieve good economic benefits and road technical performance Improve, facilitate the effect of processing and use
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] 1) Put 100 parts of 791 type SBS, 50 parts of waste engine oil, 50 parts of toluene, and 110 parts of 200# solvent oil into a sealed container in advance according to the mass ratio. After fully dissolving the SBS at room temperature, stir evenly to obtain modification Asphalt additive, spare.
[0037] 2) Take 100 parts of 70# road petroleum asphalt and heat it to a molten state, then pour it into a heating and heat preservation reactor, add 4 parts of 0# diesel oil, stir evenly, keep warm at 100-120°C, then add 0.5 parts of Yilu, 15 parts Modified asphalt additive, stir evenly, keep warm at 90-110°C, and set aside.
[0038] 3) Mix materials such as gravel and mineral powder into AC-13I-type mixture gradation, heat it to 100-120°C with an intermittent or continuous mixer, and mix according to mineral mixture: composite modified asphalt mixture = 100 : The ratio of 4.8, add the composite modified asphalt mixture and stir evenly, cool to normal temperature, and set aside...
Embodiment 2
[0045] 1) Put 100 parts of 791 type SBS, 60 parts of waste engine oil, 60 parts of toluene, and 100 parts of 200# solvent oil into a sealed container in advance according to the mass ratio. After fully dissolving the SBS at room temperature, stir evenly to obtain modification Asphalt additive, spare.
[0046]2) Take 100 parts of 70# road petroleum asphalt and heat it to a molten state, then pour it into a heating and heat preservation reactor, add 6 parts of 0# diesel oil, stir evenly, keep warm at 100-120°C, then add 1 part of Sasobit, 20 parts of modified Non-toxic asphalt additive, stir evenly, keep warm at 90-110°C, and set aside.
[0047] 3) Mix materials such as gravel and mineral powder into AC-10I type mixture gradation, heat it up to 100-120°C with batch or continuous mixer, mix according to mineral mixture: composite modified asphalt mixture = 100 : The ratio of 5.0, add the composite modified asphalt mixture and stir evenly, cool to normal temperature, and set asid...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com