Hexapeptide firming essence stock solution and preparation method thereof
A technology of hexapeptide and essence, applied in the field of hexapeptide firming essence stock solution and its preparation, can solve problems such as single effect, and achieve the effect of firming skin and eliminating fine lines
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] A hexapeptide firming essence stock solution, comprising the following raw materials in parts by weight: 1g propylene glycol, 1g butanediol, 0.01g disodium EDTA, 0.01g allantoin, 0.01g hydroxyethyl cellulose, 0.01g xanthan gum, 0.1g betaine, 0.01g hyaluronic acid, 0.5g trehalose, 0.05g carbomer, 0.05g triethanolamine, 0.1g panthenol, 0.1g nicotinamide, 0.1g hexapeptide-1, 0.5g hydrolyzed collagen, 0.01 g dipotassium glycyrrhizinate, 0.05 g phenoxyethanol and 80 g water.
[0032] Its preparation method comprises the following steps:
[0033] Step 1. Add propylene glycol, butylene glycol, disodium EDTA, allantoin, hydroxyethyl cellulose, xanthan gum, betaine, hyaluronic acid, trehalose, carbomer, and triethanolamine into the water phase pot , and add weighed water, heat up to 80°C while stirring, and stir at constant temperature for 20min until dissolved without particles;
[0034] Step 2. Turn on the cooling water to cool down to 50°C, add panthenol and nicotinamide, s...
Embodiment 2
[0037] A hexapeptide firming essence stock solution, comprising the following raw materials in parts by weight: 5g propylene glycol, 5g butanediol, 0.1g disodium EDTA, 0.3g allantoin, 0.3g hydroxyethyl cellulose, 0.3g xanthan gum, 5g Betaine, 0.05g Hyaluronic Acid, 3g Trehalose, 0.3g Carbomer, 0.3g Triethanolamine, 1g Panthenol, 0.1-1g Niacinamide, 1g Hexapeptide-1, 3g Hydrolyzed Collagen, 0.5g Glycyrrhizinate Potassium, 1 g of phenoxyethanol and 100 g of water.
[0038] Its preparation method comprises the following steps:
[0039] Step 1. Add propylene glycol, butylene glycol, disodium EDTA, allantoin, hydroxyethyl cellulose, xanthan gum, betaine, hyaluronic acid, trehalose, carbomer, and triethanolamine into the water phase pot , and add weighed water, heat up to 90°C while stirring, and stir at constant temperature for 40min until dissolved without particles;
[0040] Step 2. Turn on the cooling water to cool down to 60°C, add panthenol and nicotinamide, stir and neutral...
Embodiment 3
[0043]A hexapeptide firming essence stock solution, comprising the following raw materials in parts by weight: 2g propylene glycol, 2g butanediol, 0.02g disodium EDTA, 0.05g allantoin, 0.05g hydroxyethyl cellulose, 0.05g xanthan gum, 1g Betaine, 0.02g Hyaluronic Acid, 1g Trehalose, 0.1g Carbomer, 0.1g Triethanolamine, 0.3g Panthenol, 0.3-0.8g Niacinamide, 0.2g Hexapeptide-1, 1g Hydrolyzed Collagen, 0.05g Dipotassium glycyrrhizinate, 0.1 g phenoxyethanol and 85 g water.
[0044] Its preparation method comprises the following steps:
[0045] Step 1. Add propylene glycol, butylene glycol, disodium EDTA, allantoin, hydroxyethyl cellulose, xanthan gum, betaine, hyaluronic acid, trehalose, carbomer, and triethanolamine into the water phase pot , and add weighed water, heat up to 85°C while stirring, and stir at constant temperature for 30min until dissolved without particles;
[0046] Step 2. Turn on the cooling water to cool down to 55°C, add panthenol and nicotinamide, stir and ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com