[0015] The mass parts of each component consist of: 33 parts of epoxy resin, 78 parts of ethylene glycol, 38 parts of sodium nitrite, 27 parts of nitrilo triethanolamine, 26 parts of diatomaceous earth, 7 parts of trimethylolpropane, two 2 parts of phenylmethane diisocyanate, 3 parts of zinc phosphate, 2 parts of iron red, 5 parts of coal tar.
[0016] The preparation method is: put ethylene glycol, sodium nitrite, nitrilotriethanolamine, diatomaceous earth and trimethylolpropane into the reaction kettle, heat to 70°C, stir for 2 hours; add the reacted liquid after standing Epoxy resin, diphenylmethane diisocyanate, zinc phosphate, iron red or iron yellow, and coal tar are mixed uniformly at 100°C and then ground.
[0017] The coating can make the impact strength of the coating film reach more than 30MPa, the appearance of the coating film is smooth and bright, the adhesion is first-class, there is no abnormality in the salt spray resistance of 45 days, and the water resistanc...
Embodiment 2
[0019] The mass parts of each component consist of: 30 parts of epoxy resin, 80 parts of ethylene glycol, 40 parts of sodium nitrite, 25 parts of nitrilo triethanolamine, 25 parts of diatomaceous earth, 7 parts of trimethylolpropane, two 2 parts of phenylmethane diisocyanate, 3 parts of zinc phosphate, 2 parts of iron yellow, 6 parts of coal tar. The preparation method is the same as in Example 1.
[0020] The coating can make the impact strength of the coating film reach more than 30MPa, the appearance of the coating film is smooth and bright, the adhesion is first-class, there is no abnormality in the salt spray resistance of 45 days, and the water resistance is no abnormality of 100 days.
Embodiment 3
[0022] The mass parts of each component consist of: 35 parts of epoxy resin, 65 parts of ethylene glycol, 35 parts of sodium nitrite, 30 parts of nitrilo triethanolamine, 25 parts of diatomaceous earth, 7 parts of trimethylol propane, two 2 parts of phenylmethane diisocyanate, 3 parts of zinc phosphate, 2 parts of iron yellow, 6 parts of coal tar. The preparation method is the same as in Example 1.
[0023] The coating can make the impact strength of the coating film reach more than 30MPa, the appearance of the coating film is smooth and bright, the adhesion is first-class, there is no abnormality in the salt spray resistance of 45 days, and the water resistance is no abnormality of 100 days.
PUM
Property | Measurement | Unit |
---|---|---|
water resistance | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com