A premix and composition technology, which is applied in the directions of skin care preparations, medical preparations containing active ingredients, pharmaceutical formulas, etc., can solve the problems of difficulty in mastering the production process, low whiteness of foundation cream, and unsuitability for the entire face, etc. , to achieve the effect of simple and controllable production process, simple production process and rich and diverse colors
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0087] The surface treatment of embodiment 1 titanium dioxide
[0088] Example 1a Surface treatment of titanium dioxide using triethoxymethylsilane as the first siloxane surface treatment agent
[0089] Mix 0.45 kg of triethoxymethylsilane (ie, n1=2, a1=1 in formula (A)) and 1.05 kg of ethanol (95%) to prepare the first surface treatment solution. Ready to use.
[0090] Add 15kg of titanium dioxide into the mixer, and under stirring, spray the pre-prepared first surface treatment solution into the mixer and stir thoroughly, so that the first surface reaction solution and titanium dioxide are evenly mixed to obtain the first material.
[0091] The first material was discharged, immediately sent to an oven, baked at 105° C. for 4 hours, cooled naturally and discharged.
[0092] The reaction process comprises the steps: (1) triethoxymethylsilane hydrolysis see Figure 2A and (2) hydroxyl condensation dehydration see Figure 2B . After treatment, the surface properties of the...
Embodiment 2
[0108] The processing of embodiment 2 inorganic pigment iron oxides
Embodiment 2a
[0109] Embodiment 2a uses trimethoxyhexadecylsilane to carry out surface treatment to iron oxide black
[0110] Mix 0.45kg of trimethoxyhexadecylsilane (in formula (F), n6=16, a6=1, m6=1) and 1.05kg of 95° alcohol to prepare the second surface treatment liquid. Ready to use.
[0111] Add 15kg of iron oxide black into the mixer, and under stirring, spray the pre-prepared second surface treatment liquid into the mixer and fully stir, so that the second surface treatment liquid and iron oxide black are evenly mixed to obtain the second material .
[0112] The second material was discharged, immediately sent to an oven, baked at 105° C. for 4 hours, cooled naturally and discharged.
[0113] The reaction process comprises the steps: (1) trimethoxyhexadecylsilane hydrolysis (see Figure 6A ); (2) hydroxyl condensation dehydration (see Figure 6B ). After treatment, the chemical properties of the iron oxide powder surface are as follows: Figure 6C shown. After treatment by th...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com