A production process and high-elasticity technology, used in biochemical fiber treatment, enzyme/microorganism biochemical treatment, dry cleaning fiber products, etc., can solve the problems of serious environmental pollution, large fiber damage, low fabric strength, etc., to reduce pollution and production. Low cost and good flexibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] see figure 1 , the present invention provides a technical solution: a production process of high elasticity and low shrinkage pure cotton interlining, comprising the following steps:
[0027] A. Weaving: Weaving the sizing-treated cotton yarn into gray cloth;
[0028] B, singeing: adopt gas singeing machine to carry out singeing process to the gray cloth that step A obtains, remove the hairiness on its surface;
[0029] C, desizing: desizing the gray cloth after step B singeing, removing the size on the yarn surface;
[0030] D, cold stacking: roll the gray cloth after the desizing treatment in step C on a coiling machine, and then stack it after wrapping it with a plastic film; stack it for 2 hours;
[0031] E. Washing: wash the gray fabrics stacked in step D with hot water and cold water; the temperature of the hot water is 60°C, and the washing time is 5 minutes; the temperature of the cold water is 15°C, and the washing time is 10 minutes;
[0032] F, oxygen blea...
Embodiment 2
[0044] The present invention provides a technical solution: a production process of high-elasticity and low-shrinkage pure cotton interlining, comprising the following steps:
[0045] A. Weaving: Weaving the sizing-treated cotton yarn into gray cloth;
[0046] B, singeing: adopt gas singeing machine to carry out singeing process to the gray cloth that step A obtains, remove the hairiness on its surface;
[0047] C, desizing: desizing the gray cloth after step B singeing, removing the size on the yarn surface;
[0048] D, cold stacking: the gray cloth after the desizing treatment in step C is coiled on a coiler, and then stacked after being wrapped in a plastic film; stacked for 4h;
[0049] E. Washing: wash the gray fabrics stacked in step D with hot water and cold water; the temperature of the hot water is 80°C, and the washing time is 5 minutes; the temperature of the cold water is 25°C, and the washing time is 20 minutes;
[0050] F, oxygen bleaching: put the gray cloth a...
Embodiment 3
[0062] The present invention provides a technical solution: a production process of high-elasticity and low-shrinkage pure cotton interlining, comprising the following steps:
[0063] A. Weaving: Weaving the sizing-treated cotton yarn into gray cloth;
[0064] B, singeing: adopt gas singeing machine to carry out singeing process to the gray cloth that step A obtains, remove the hairiness on its surface;
[0065] C, desizing: desizing the gray cloth after step B singeing, removing the size on the yarn surface;
[0066] D, cold stacking: the gray cloth after the desizing treatment in step C is coiled on a coiler, and then stacked after being wrapped with a plastic film; stacked for 2-4h;
[0067] E. Washing: wash the gray fabrics stacked in step D with hot water and cold water; the temperature of the hot water is 65°C, and the washing time is 5 minutes; the temperature of the cold water is 17°C, and the washing time is 12 minutes;
[0068] F, oxygen bleaching: put the gray cloth...