A filter and formaldehyde technology, which is applied in the field of formaldehyde removal coating and formaldehyde removal filter, can solve the problems that cannot meet the requirements of the national standard, the performance parameters are far from each other, and cannot play the role of formaldehyde removal, so as to achieve guaranteed effect and prevent Shedding effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] Embodiment 1, a formaldehyde removal filter of the present invention, a formaldehyde removal catalyst coating and a catalyst fixing layer are arranged on the carrier, and the catalyst fixing layer is arranged on the outer layer of the catalyst coating.
[0026] The composition of the formaldehyde removal catalyst coating is: 30% of manganese dioxide with a particle size of 50 nanometers, 0.1% of nano-platinum with a particle size of 10 nanometers, 20% of acrylic adhesive, mixed with 49.9% of water, and stirred for 60 minutes to make it evenly mixed .
[0027] The catalyst fixing layer is composed of: 25% water-based polyurethane adhesive, 0.2% cellulose thickener, 2% brown powder, mixed with 72.8% water and stirred evenly, the viscosity is 1200mPa·s.
[0028] Add the prepared catalyst coating to the ceramic honeycomb carrier by spraying, then dry it in a vacuum oven, and then use a roller to evenly coat the catalyst fixed layer prepared above on the catalyst coating. I...
Embodiment 2
[0031] Embodiment 2, a formaldehyde removal filter of the present invention, a formaldehyde removal catalyst coating and a catalyst fixing layer are arranged on the carrier, and the catalyst fixing layer is arranged on the outer layer of the catalyst coating.
[0032] The composition of the formaldehyde removal catalyst coating is: 10% titanium dioxide with a particle size of 30 nanometers, 2% nano-palladium with a particle size of 20 nanometers, 5% cerium oxide with a particle size of 30 nanometers, 31% EVA adhesive, mixed with 52% water , and stir for 60 minutes to mix well.
[0033] The composition of the catalyst fixing layer is: 30% of acrylic adhesive, 0.1% of cellulose thickener, mixed with 69.9% of water and stirred evenly, the viscosity is 1500mPa·s.