[0010] Embodiment: a kind of preparation technology of topcoat comprises the following steps,
[0011] a. Add 40-80 parts of water, 85-130 parts of polyethylene oxide, 140-170 parts of glycidyl methacrylate and 90-140 parts of toner into the mixer in order, mix and stir, and keep the mixer at 650-750 rpm minutes, stirring for 5 minutes;
[0012] b. Adjustment Adjust the speed of the mixer to 1800-1900 rpm, and then add 75-85 parts of polyethylene terephthalate, 20-40 parts of polyphenylene sulfide, and 25-50 parts of acrylamide in sequence, Disperse at high speed for 30 minutes;
[0013] c. After dispersion, the paint is obtained, and its fineness is less than 60 microns;
[0014] d. Put the paint in cans, seal and pack.
[0015] As preferably, when stirring, the stirrer is reversed once every 5 minutes.
[0016] The invention has excellent heat resistance, comprehensive chemical stability and heat resistance, can still work normally below 200 DEG C, and has good stability...