A self-compacting concrete preparation process and special modified admixture preparation
A technology of self-compacting concrete and admixture, applied in the field of self-compacting concrete, can solve problems such as lack of auxiliary materials, and achieve the effects of reducing distance, enhancing structural strength, and enhancing bulk density
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0055] A special additive preparation process, including water, organic solvent, emulsifier, nylon powder, EVA powder, agave powder, titanium dioxide, aluminum sulfate, light stabilizer, heat stabilizer.
[0056] Include 20 parts of water, 10 parts of organic solvent, 8 parts of emulsifier, 0.8 part of EVA powder, 3 parts of nylon powder, 7 parts of agave powder, 1.2 parts of titanium dioxide, 0.3 part of aluminum sulfate, 1 part of heat stabilizer in the present embodiment and 1 part light stabilizer.
[0057] The preparation method is as follows:
[0058] S1: Dissolving EVA powder in an organic solvent;
[0059] S2: Pour in water and emulsifier, and stir at high speed to form an emulsified suspension;
[0060] S3: Soak the agave powder in clean water for 30-40 minutes, drain the water, mix it evenly with the nylon powder and introduce it into the emulsified suspension;
[0061] S4: Pour titanium dioxide, aluminum sulfate, heat stabilizer, light stabilizer into it and mix ...
Embodiment 6
[0066] A self-compacting concrete preparation process, including water, cement, fly ash, mineral powder, medium sand, crushed stone, dispersant, thickener, and water reducer; wherein, the crushed stone adopts stones with a particle size of 5-10mm .
[0067]Include 160 parts of water, 250 parts of cement, 115 parts of fly ash, 38, mineral powder, 1000 parts of medium sand, 800 parts of gravel, 0.5 part of dispersant, 0.01 part of thickener, 7.5 parts of water reducer in this embodiment ; Also includes 0.005% special modified admixture.
[0068] Self-compacting concrete is prepared as follows:
[0069] Step 1: Pour 10-20 parts of water into the high-speed mixer for wetting;
[0070] Step 2: Pour the dispersant, water reducer, and special modified admixture into it and mix evenly;
[0071] Step 3: Add crushed stone and medium sand and stir evenly;
[0072] Step 4: Pour in the remaining water and keep stirring;
[0073] Step 5: Pour in cement, fly ash and mineral powder, and ...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com