Brightener for numerical control ironing machine and preparation method of brightener
A technology for ironing machines and brighteners, which is applied in the field of brightener materials, and can solve problems such as insufficient surface brightness and increased maintenance costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0014] The invention provides a preparation method of a brightener for a numerically controlled ironing machine, wherein the preparation method comprises:
[0015] 1) In the presence of a solvent, mix polyether-modified heptamethyltrisiloxane and sodium dihydrogen phosphate to prepare a mixed solution M1;
[0016] 2) Mix the mixed liquid M1 prepared in step 1), sodium benzoate, nonylphenol polyoxyethylene ether, o-chlorobenzaldehyde and cinnamic acid to prepare a mixture M2;
[0017] 3) Under the condition of pH 4-6, ethylene glycol monobutyl ether is added to the mixture M2 and mixed to prepare a brightener for a numerically controlled ironing machine.
[0018] The present invention mixes polyether-modified heptamethyltrisiloxane and sodium dihydrogen phosphate, then mixes the above mixed solution with sodium benzoate, nonylphenol polyoxyethylene ether, o-chlorobenzaldehyde and cinnamic acid, and further, Under the condition of pH 4-6, ethylene glycol monobutyl ether is adde...
Embodiment 1
[0031] 1) In the presence of 1000 parts by weight of water, mix 10 parts by weight of polyether-modified heptamethyltrisiloxane and 5 parts by weight of sodium dihydrogen phosphate to prepare a mixed solution M1;
[0032] 2) The mixed solution M1, 5 parts by weight of sodium benzoate, 10 parts by weight of nonylphenol polyoxyethylene ether, 10 parts by weight of o-chlorobenzaldehyde and 5 parts by weight of cinnamic acid prepared in the step 1) of 1000 parts by weight are placed in Mixing at a temperature of 30°C for 10 minutes and then mixing at a temperature of 60°C for 10 minutes to obtain a mixture M2;
[0033] 3) Under the condition of pH 4, 5 parts by weight of ethylene glycol monobutyl ether was added to 1000 parts by weight of the mixture M2 and mixed to prepare brightener A1 for CNC ironing machine.
Embodiment 2
[0035] 1) In the presence of 1000 parts by weight of water, mix 60 parts by weight of polyether-modified heptamethyltrisiloxane and 30 parts by weight of sodium dihydrogen phosphate to prepare a mixed solution M1;
[0036] 2) The mixed solution M1, 15 parts by weight of sodium benzoate, 30 parts by weight of nonylphenol polyoxyethylene ether, 20 parts by weight of o-chlorobenzaldehyde and 10 parts by weight of cinnamic acid prepared in the step 1) of 1000 parts by weight are placed in Mixing was carried out at a temperature of 50°C for 30 minutes, and then mixed at a temperature of 70°C for 20 minutes to obtain a mixture M2;
[0037] 3) Under the condition of pH 6, 20 parts by weight of ethylene glycol monobutyl ether was added to 1000 parts by weight of the mixture M2 and mixed to prepare brightener A2 for CNC ironing machine.
PUM