Method for cementing and filling of metal mine by application of phosphogypsum material
A gypsum material and cemented filling technology, which is applied in the field of cemented filling of metal mines with phosphogypsum material, can solve the problems of land occupation and surrounding environmental pollution, and achieve the effects of high energy saving efficiency, safe operation and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0026] 2) Preparation of phosphogypsum cementitious material: mixing phosphogypsum, slag, steel slag and water reducing agent in a mixer to obtain phosphogypsum cementitious material;
[0027] 3) Preparation of phosphogypsum dry mix: mixing and stirring the graded tailings and phosphogypsum cementitious material in a mixer to obtain phosphogypsum dry mix;
[0028] 4) Preparation of phosphogypsum filling slurry: mixing and stirring phosphogypsum dry mix and water in a secondary mixer to obtain phosphogypsum filling slurry;
[0029] 5) Filling: The phosphogypsum filling slurry is self-flowed to the mining empty area through the filling pipeline. When the filling height of the slurry reaches the drainage and exhaust outlet, the drainage and exhaust pipeline is blocked, the slurry supply is stopped, and the filling pipeline is cut off.
[0030] Preferably, in step 1), the width of the retaining wall is >50cm.
[0031] Preferably, in step 1), the retaining wall is covered with con...
Embodiment
[0041] 1. Preparation of filling site
[0042] Connect one end of the filling pipe to the outlet of the secondary mixer, and the other end to the mining vacancy to be filled along the mine shaft and mining passage, and place the outlet at the highest point of the mining vacancy; clean up the site and take out all useful items , and then build a wall with bricks and cement, build a pipe with a diameter of about 5cm on the top of the retaining wall for drainage and exhaust, and seal the opening of the mining empty area. The width of the retaining wall should be at least greater than 50cm to prevent the wall If it collapses, put a layer of concrete about 5cm thick on the wall to increase the impact resistance of the retaining wall and prevent water seepage.
[0043] 2. Preparation of phosphogypsum cementitious material
[0044] Add 70 parts by mass of phosphogypsum, 14.5 parts by mass of slag, 15 parts by mass of steel slag and 0.5 parts by mass of water reducing agent into the ...