A kind of hydrophilic anti-oxidation inhibitor for mine and preparation method thereof
An antioxidant and inhibitor technology, which is used in mining equipment, earth-moving drilling, fire protection equipment, etc., can solve the problems of rare physical and chemical synergistic resistance type inhibitor, lack of chemical inhibitor, and high cost. Low compounding cost, delayed water loss, low cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029]A hydrophilic anti-oxidation inhibitor for mines is prepared from polymer base material, organic antioxidant, fire extinguishing agent, coagulant and water as raw materials. The raw materials for the preparation of the polymer base material are polyacrylic acid, sodium alginate and water; the organic antioxidant is melatonin; the fire extinguishing agent is ammonium dihydrogen phosphate; and the coagulation accelerator is ammonium bicarbonate. During the preparation of the polymer base material, the mass ratio of polyacrylic acid, sodium alginate and water is 1:1.5:2; the inhibitor is prepared from the polymer base material, organic antioxidant, fire extinguishing agent, coagulant and water In the process, the mass ratio of organic antioxidant to polymer base material is 1:7, the mass ratio of organic antioxidant to fire extinguishing agent is 1:3, the mass ratio of organic antioxidant to coagulant is 1:5, and the mass ratio of organic antioxidant to coagulant is 1:5. Th...
Embodiment 2
[0032] A hydrophilic anti-oxidation inhibitor for mining is composed of a polymer base material, an organic antioxidant, a fire extinguishing agent, a coagulant and water. The polymer base material is polyacrylic acid, sodium alginate and water; the organic antioxidant is melatonin; the fire extinguishing agent is ammonium dihydrogen phosphate; and the coagulation accelerator is ammonium bicarbonate. During the preparation of the polymer base material, the mass ratio of polyacrylic acid, sodium alginate and water is 1:2:3; the inhibitor is prepared from the polymer base material, organic antioxidant, fire extinguishing agent, coagulant and water In the process, the mass ratio of organic antioxidant to polymer base material is 1:6, the mass ratio of organic antioxidant to fire extinguishing agent is 1:3.5, the mass ratio of organic antioxidant to coagulant is 1:6, and the organic The mass ratio of the total mass of antioxidant, polymer base material, fire extinguishing agent an...
Embodiment 3
[0035] A hydrophilic anti-oxidation inhibitor for mining is composed of a polymer base material, an organic antioxidant, a fire extinguishing agent, a coagulant and water. The polymer base material is polyacrylic acid, sodium alginate and water; the organic antioxidant is melatonin; the fire extinguishing agent is ammonium dihydrogen phosphate; and the coagulation accelerator is ammonium bicarbonate. During the preparation of the polymer base material, the mass ratio of polyacrylic acid, sodium alginate and water is 1:2.5:3; the polymer base material, organic antioxidant, fire extinguishing agent, coagulant and water are used as raw materials to prepare the chemical inhibitor In the process, the mass ratio of organic antioxidant to polymer base material is 1:5, the mass ratio of organic antioxidant to fire extinguishing agent is 1:4, and the mass ratio of organic antioxidant to coagulant accelerator is 1:7. The mass ratio of the total mass of molecular base material, organic a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com