Problems solved by technology
Method used
Examples
Embodiment Construction
[0010] 30 kg of dehydrated malic acid resin, 10 kg of propylene glycol, 0.01 kg of polyethylene glycol (600), 1 kg of ultrafine silicon dioxide, 2 kg of polyamide wax (n-butanol, naphtha mixture), 1250 mesh of talcum powder 2 kg, 15 kg of o-phthalic unsaturated polyester resin, 0.1 kg of polyvinyl butyral, 10 kg of styrene, and 2 kg of selenium photoplastic initiator (D1173). Acid resin polymer (solid content 80%), propylene glycol, polyethylene glycol (600), ultrafine silicon dioxide, polyamide wax (n-butanol, petroleum naphtha mixture), talcum powder 1250 mesh, and continue to stir for 90 minutes , then add o-phthalic unsaturated polyester resin, polyvinyl butyral, styrene, polyether modified polydimethylsiloxane, continue stirring for 30 minutes, and finally add selenium photoplastic initiator (D1173), Pay attention to avoid light.
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com