[0023] A processing method for weaving rattan, comprising the following steps:
[0024] 1) Rattan pretreatment: classify and pick rattan, and classify rattan in different diameter ranges;
[0025] 2) rattan treatment: polish the sorted treatment, and polish off the scars and protrusions on the surface of the rattan;
[0026] 3) Preparation of soaking solution: soaking solution consists of 2-3 parts of tartaric acid, 2-3 parts of sodium chloride, 60-70 parts of water; 1 part of boric acid, 6 parts of glycerin, 1-2 parts of chlorbacteric acid, melamine cyanuric acid Composed of 1-2 parts of salt and 3-4 parts of potassium gold chloride;
[0027] 4) Initial soaking: Pour the prepared soaking solution into the soaking tank, then put the polished rattan, heat the soaking solution, and keep it warm for 10-30 minutes when heated to 40-50°C;
[0028] 5) Pre-drying treatment: put the soaked rattan into an environment with a temperature of 40° C. and a relative humidity of 30% to air-...
Embodiment 2
[0041] A processing method for weaving rattan, comprising the following steps:
[0042] 1) Rattan pretreatment: classify and pick rattan, and classify rattan in different diameter ranges;
[0043] 2) rattan treatment: polish the sorted treatment, and polish off the scars and protrusions on the surface of the rattan;
[0044] 3) Preparation of soaking solution: soaking solution consists of 2-3 parts of tartaric acid, 2-3 parts of sodium chloride, 60-70 parts of water; 1 part of boric acid, 6 parts of glycerin, 1-2 parts of chlorbacteric acid, melamine cyanuric acid Composed of 1-2 parts of salt and 3-4 parts of potassium gold chloride;
[0045] 4) Initial soaking: Pour the prepared soaking solution into the soaking tank, then put the polished rattan, heat the soaking solution, and keep it warm for 10-30 minutes when heated to 40-50°C;
[0046] 5) Pre-drying treatment: put the soaked rattan into an environment with a temperature of 55°C and a relative humidity of 40% for 2 hou...