Special environment-friendly binder for wooden furniture and method for preparing special environment-friendly binder
A wooden furniture and adhesive technology, applied in the direction of lignin adhesive, adhesive, adhesive type, etc., can solve the problems of high production cost and weak adhesive force, and achieve low cost, simple preparation method, Excellent adhesive effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] 1. Dissolve 40 parts of lignin, 20 parts of konjac gum and 15 parts of oxidized starch in 68 parts of water and mix evenly, then add 3 parts of boric acid and heat to 90°C; react for 15 minutes;
[0024] 2. Add 9 parts of pine oil and 4 parts of tung oil to the mixed solution after the reaction in step 1, and react for 30 minutes at 320°C and 2 atmospheres;
[0025] 3. After the reaction is completed, cool down to 140°C, add 7 parts of emulsifier for emulsification treatment for 5 minutes, and cool to obtain a binder.
Embodiment 2
[0027] 1. Dissolve 35 parts of lignin, 25 parts of konjac gum and 18 parts of oxidized starch in 65 parts of water and mix evenly, then add 4 parts of boric acid and heat to 95°C; react for 10 minutes;
[0028] 2. Add 8 parts of pine oil and 5 parts of tung oil to the mixed solution after the reaction in step 1, and react at 350°C and 3 atmospheres for 25 minutes;
[0029] 3. After the reaction is completed, cool down to 150°C, add 5 parts of emulsifier for emulsification treatment for 3 minutes, and cool to obtain a binder.
Embodiment 3
[0031] 1. Dissolve 45 parts of lignin, 18 parts of konjac gum and 18 parts of oxidized starch in 65 parts of water and mix evenly, then add 2 parts of boric acid and heat to 95°C; react for 20 minutes;
[0032] 2. Add 8 parts of pine oil and 3-5 parts of tung oil to the mixed solution after the reaction in step 1, and react at 350°C and 1 atmospheric pressure for 25 minutes;
[0033] 3. After the reaction is completed, cool down to 120°C, add 8 parts of emulsifier for emulsification treatment for 8 minutes, and cool to obtain a binder.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com