A stage and humidity technology, applied in wood treatment, pressure impregnation, wood processing equipment, etc., can solve the problems of harm to the human body, failure to achieve good results, strong irritation, etc., to achieve easy weaving, reduced fracture rate, The effect of improving processing efficiency

Inactive Publication Date: 2018-12-07
ANHUI HUAYU CRAFTS GRP
View PDF5 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] Due to the characteristics of willow weaving itself, it is relatively hard in the weaving process, which is not conducive to weaving, and needs to be softened. At present, the softening is mainly the traditional method, such as soaking in boiling water, boiling, etc., which is not only time-consuming but also fails to achieve a good result. As a result, although various softening treatment liquids created by people recently can achieve better softening effects, such softening treatment liquids are usually highly irritating, harmful to the human body, and will also affect the characteristics of willow itself.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0016] A method for softening bark willow for weaving, comprising the following content:

[0017] (1) Wash the willows without pests and diseases and soak them in sulfuric acid solution with a mass concentration of 15% for 35 minutes, and peel them for later use after soaking;

[0018] (2) Dry the peeled willows in three stages, the first stage drying temperature is 60°C, the humidity is 75%, and the drying time is 12 minutes; the second stage temperature is 88°C, humidity is 60%, The drying time is 8 minutes; in the third stage, the temperature is 75°C, the humidity is 50%, and the drying time is 25 minutes;

[0019] (3) After soaking the above-mentioned dried willow bark with biomass treatment solution, pressurize to 2.5MPa in a closed tank, and keep the pressure for 2 hours to obtain it;

[0020] The preparation method of the biomass treatment solution is as follows: mix litchi peel, wheat straw and okra in a volume ratio of 18:40:1, then add dimethylacetamide equivalent t...

Embodiment 2

[0027] A method for softening bark willow for weaving, comprising the following content:

[0028] (1) Wash the willows without pests and diseases and soak them in sulfuric acid solution with a mass concentration of 12% for 40 minutes, and peel them for later use after soaking;

[0029] (2) Dry the above peeled willows in three stages, the first stage drying temperature is 55°C, the humidity is 75%, and the drying time is 10 minutes; the second stage temperature is 85°C, humidity is 60%, The drying time is 10 minutes; in the third stage, the temperature is 70°C, the humidity is 50%, and the drying time is 20 minutes;

[0030] (3) After soaking the above-mentioned dried willow bark in a biomass treatment solution, pressurize to 3MPa in a closed tank, and hold the pressure for 2 hours to obtain it;

[0031] The preparation method of the biomass treatment solution is as follows: mix litchi peel, wheat straw and okra in a volume ratio of 20:45:1, then add dimethylacetamide equival...

Embodiment 3

[0038] A method for softening bark willow for weaving, comprising the following content:

[0039] (1) Wash the willows without pests and diseases and soak them in sulfuric acid solution with a mass concentration of 18% for 30 minutes, and peel them for later use after soaking;

[0040] (2) Dry the peeled willow bark in three stages, the first stage drying temperature is 65°C, the humidity is 75%, and the drying time is 15 minutes; the second stage temperature is 90°C, humidity is 60%, The drying time is 6 minutes; in the third stage, the temperature is 80°C, the humidity is 50%, and the drying time is 30 minutes;

[0041] (3) After soaking the above-mentioned dried willow bark in a biomass treatment solution, pressurize to 2MPa in a closed tank, and hold the pressure for 2 hours to obtain it;

[0042] The preparation method of the biomass treatment liquid is as follows: mix litchi peel, wheat straw and okra with a volume ratio of 16:35:1, then add dimethylacetamide equivalent...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention belongs to the technical field of purple willow processing, and particularly relates to a softening method for a purple willow for knitting. The purple willow free of plant diseases andinsect pests is cleaned and then soaked for 30 to 40 minutes with a sulfuric acid solution with the mass concentration being 12 to 18%, after peeling, the purple willow is dried in three stages, the dried purple willow is soaked through biomass treatment fluid, in a seal tank, pressurizing to 2 to 3 MPa is carried out, and after pressure maintaining is carried out for two hours, the willow is dried until the water containing amount is lower than 10%. Compared with the prior art, the method has the beneficial effects that through sulfuric acid solution treatment, peeling is assisted, drying iscarried out in three stages, the purple willow of certain toughness is obtained, the biomass treatment fluid is used for treating, drying is carried out again, the purple willow is further softened, knitting is easily achieved, during machining, the breakage rate is reduced, and the machining efficiency is improved.

Description

technical field [0001] The invention belongs to the technical field of bark willow processing, in particular to a softening method of bark willow for weaving. Background technique [0002] Willow is one of the traditional Chinese handicrafts, rich in raw material resources and with a long history. Willow woven products are beautiful in appearance, low in price, green and environmentally friendly, and have good artistry and practicability. They are widely used in daily life, home decoration, and art appreciation. They are welcomed by domestic and foreign consumers and have a good market prospect. Willow is one of the main raw materials for making willow. [0003] Due to the characteristics of willow weaving itself, it is relatively hard in the weaving process, which is not conducive to weaving, and needs to be softened. At present, the softening is mainly the traditional method, such as soaking in boiling water, boiling, etc., which is not only time-consuming but also fails ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): B27K5/06B27K3/10B27K5/04
CPCB27K3/10B27K5/04B27K5/06
Inventor 王东营
Owner ANHUI HUAYU CRAFTS GRP
Features
  • R&D
  • Intellectual Property
  • Life Sciences
  • Materials
  • Tech Scout
Why Patsnap Eureka
  • Unparalleled Data Quality
  • Higher Quality Content
  • 60% Fewer Hallucinations
Social media
Patsnap Eureka Blog
Learn More