Anti-static anti-corrosive paint using aluminum triphosphate/nano-silver compound electric conducting powder
A technology of composite conductive powder and aluminum tripolyphosphate, which is applied in the direction of anti-corrosion coatings, conductive coatings, epoxy resin coatings, etc., can solve the problems such as the antistatic performance and influence of coatings that have not been investigated, and achieve long-lasting anti-corrosion performance, simple preparation process, The effect of small resistivity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0030] The preparation of coating comprises the following steps:
[0031] (1) Take each component according to the ratio, and add deionized water, dipropylene glycol methyl ether, propylene glycol butyl ether, BYK190, BYK024, aluminum tripolyphosphate / nano-silver composite conductive powder to the material tank of the disperser in sequence body, titanium dioxide, barium sulfate and talc powder, disperse at a speed of 1000-2000rpm for 30-60min; (2) reduce the speed of the disperser to 300-800rpm, add water-based epoxy resin, and continue stirring for 20-40min to obtain component A (3) When in use, take the B component according to the weight ratio and add it to the A component, and get the antistatic anticorrosion coating after stirring evenly.
[0032] When testing the performance of the paint, test the salt spray resistance of the paint according to the HG / T 4759-2014 standard, and use the surface resistance tester to test the surface resistance of the coating.
[0033] The ...
PUM
| Property | Measurement | Unit |
|---|---|---|
| Salt spray resistance | aaaaa | aaaaa |
| Surface resistance | aaaaa | aaaaa |
| Salt spray resistance | aaaaa | aaaaa |