Warm-keeping and health-care flyknit vamp and production method thereof
A shoe upper and flying weaving technology, which is applied to shoe uppers, footwear, braided fabrics, etc., can solve the problems of poor functionality, unfavorable strength of flying weaving uppers, and affecting the quality of flying weaving uppers, so as to improve the heat preservation effect, Easy to operate, energy-enhancing effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] The flying woven shoe upper for keeping warm and keeping healthy in this embodiment comprises the first yarn and the second yarn woven according to the computer software program, the first yarn is made of rubber silk as the core and twisted by double fiber layers The second yarn is made of rubber silk as the core and twisted with a fiber layer and an alkene-based fiber layer. The alkene-based fiber layer includes graphene oxide fibers and graphene oxide fibers bonded Hot lava and mocha sand.
[0032] In this embodiment, in the first yarn, the double-ply fiber layer is twisted with the rubber yarn in the z direction, and the twisting in the z direction can improve the air permeability of the shoe upper.
[0033] In this embodiment, in the first yarn, the fibers of the double-ply fiber layer are polyester filaments or nylon filaments.
[0034] In this embodiment, in the second yarn, one fiber layer and one alkene-based fiber layer are twisted with the rubber yarn in the ...
Embodiment 2
[0037] The preparation method of a kind of warm-keeping, health-care flying woven shoe upper in this embodiment comprises the following steps:
[0038] Step 1: Preparation of Alkene-based Fibers
[0039] 1) Grinding: Using hot lava and mocha sand, firstly grind the hot lava and mocha sand into powder respectively, then mix the two and continue grinding to obtain nano-scale mixed powder of hot lava and mocha sand. The powder is dried for use, wherein the weight ratio of hot lava to mocha sand is 0.5:2;
[0040] 2) Preparation of carboxylated graphene oxide:
[0041] a, adopt the graphene oxide of formula quantity, add water to it, the graphene oxide mixed with water is ultrasonically vibrated under water bath condition, and water bath temperature is 40 ℃, be stirred simultaneously, so that improve the dispersion degree of graphene oxide in water, Obtain a uniformly dispersed mixture of water and graphene oxide;
[0042] b. Add NaOH to the above-mentioned mixture of water and...
Embodiment 3
[0051] In this embodiment, a method for preparing a warm-keeping, health-care flying woven shoe upper includes the following steps:
[0052] Step 1: Preparation of Alkene-based Fibers
[0053]1) Grinding: Using hot lava and mocha sand, firstly grind the hot lava and mocha sand into powder respectively, then mix the two and continue grinding to obtain nano-scale mixed powder of hot lava and mocha sand. The powder is dried for use, and the weight ratio of hot lava to mocha sand is 1:2.
[0054] 2) Preparation of carboxylated graphene oxide:
[0055] a, adopt the graphene oxide of formula quantity, add water to it, the graphene oxide mixed with water is ultrasonically vibrated under water bath condition, and water bath temperature is 30 ℃, be stirred simultaneously, so that improve the dispersion degree of graphene oxide in water, Obtain a uniformly dispersed mixture of water and graphene oxide;
[0056] b. Add NaOH to the above-mentioned mixture of water and graphene oxide, s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com