Cool and comfortable fabric
A comfortable and fabric technology, applied in the direction of clothing, yarn, protective clothing, etc., can solve the problems of poor hygroscopicity, easy breeding of bacteria, poor light resistance of fabrics, etc., and achieve the effects of ensuring health, excellent moisture absorption and moisture conductivity, and overcoming easy wrinkling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0109] A second aspect of the present invention provides a method for preparing a cool and comfortable fabric, comprising the steps of:
[0110] (1) Mix polypropylene, epoxy resin, and coffee carbon fiber evenly;
[0111] (2) Add polyvinyl alcohol, modified silicone oil, thiazole compound, cyclodextrin, binder, surfactant to the mixture in step (1), add 20-40 parts by weight of water, stir and heat to a molten state ;
[0112] (3) Send the molten matter of step (2) to the spinning box through the melt pipeline, extrude from the spinneret to form fibers, and then blend with jade fibers to obtain the fabric;
[0113] The spinning temperature of the spinning box is 270-300° C., and the spinning speed is 3000-3500 m / min.
Embodiment 1
[0118] Embodiment 1 provides a cool and comfortable fabric, which at least includes the following components in parts by weight: 30 parts of polypropylene, 60 parts of epoxy resin, 40 parts of jade fiber, 20 parts of coffee carbon fiber, 10 parts of polyvinyl alcohol, 10 parts of modified silicone oil, 4 parts of thiazole ring compound, 3 parts of cyclodextrin, 2 parts of adhesive, 1 part of surfactant;
[0119] Described polypropylene is syndiotactic polypropylene, and trade mark is SPP 208;
[0120] Described epoxy resin is diglycidyl tetrahydrophthalate;
[0121] Described jade fiber is the short fiber of jade fiber of (1.4-4.5) dtex * (32-114) mm;
[0122] The coffee carbon fiber is 1.5D-10D, 38mm-42mm, hollow round hole, special-shaped coffee carbon fiber;
[0123] The polyvinyl alcohol is PVA 217;
[0124] The modified silicone oil is a compound of primary amino-modified silicone oil and epoxy-polyether modified silicone oil; and the grade of the primary amino-modifie...
Embodiment 2
[0135] Embodiment 2 provides a cool and comfortable fabric, which at least includes the following components in parts by weight: 50 parts of polypropylene, 80 parts of epoxy resin, 50 parts of jade fiber, 40 parts of coffee carbon fiber, 20 parts of polyvinyl alcohol, 20 parts of modified silicone oil, 12 parts of thiazole ring compound, 6 parts of cyclodextrin, 5 parts of adhesive, 3 parts of surfactant;
[0136] Described polypropylene is syndiotactic polypropylene, and trade mark is SPP 208;
[0137] Described epoxy resin is diglycidyl tetrahydrophthalate;
[0138] Described jade fiber is the short fiber of jade fiber of (1.4-4.5) dtex * (32-114) mm;
[0139] The coffee carbon fiber is 1.5D-10D, 38mm-42mm, hollow round hole, special-shaped coffee carbon fiber;
[0140] The polyvinyl alcohol is PVA 217;
[0141] The modified silicone oil is the same as Example 1, except that the weight portion of the primary amino-modified silicone oil is 16 parts, and the weight portion ...