A construction method and cement mortar technology, which are applied in construction, building construction, covering/lining, etc., can solve problems such as poor compatibility of the base layer, easy aging, environmental pollution, etc., and achieve a significant reduction in waterproof effect and good compatibility. , Improve the effect of water penetration resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0038] A wall construction method includes the following steps:
[0039] S1 grassroots treatment: chisel the unevenness of the wall to clean up dust and impurities; soak the wall with water to control the moisture content of the wall to 12wt%;
[0040] S2: Apply cement mortar for the first time, flatten the mortar with a pressure ruler, control the thickness of the cement mortar to 5mm, and cure for 60 minutes; apply the cement mortar for the second time, flatten the mortar with a pressure ruler, and control the cement mortar The thickness of the cement mortar is controlled at 5mm and cured for 60 minutes; the third time the cement mortar is applied, the mortar is flattened with a pressure ruler, and the thickness of the cement mortar is controlled at 8mm and cured for 48 hours;
[0041] S3 brushing super-hydrophobic emulsion: spray super-hydrophobic emulsion on the surface of the cured cement mortar, the dosage is 250g / m 2 , Cured for 7 days under the conditions of air humidity 75% ...
Embodiment 2
[0045] A wall construction method includes the following steps:
[0046] S1 grassroots treatment: chisel the unevenness of the wall to clean up dust and impurities; soak the wall with water to control the moisture content of the wall to 12wt%;
[0047] S2: Apply cement mortar for the first time, flatten the mortar with a pressure ruler, control the thickness of the cement mortar to 5mm, and cure for 60 minutes; apply the cement mortar for the second time, flatten the mortar with a pressure ruler, and control the cement mortar The thickness of the cement mortar is controlled at 5mm and cured for 60 minutes; the third time the cement mortar is applied, the mortar is flattened with a pressure ruler, and the thickness of the cement mortar is controlled at 8mm and cured for 48 hours;
[0048] S3 brushing super-hydrophobic emulsion: spray super-hydrophobic emulsion on the surface of the cured cement mortar, the dosage is 250g / m 2 , Cured for 7 days under the conditions of air humidity 75% ...
Embodiment 3
[0054] A wall construction method includes the following steps:
[0055] S1 grassroots treatment: chisel the unevenness of the wall to clean up dust and impurities; soak the wall with water to control the moisture content of the wall to 12wt%;
[0056] S2: Apply cement mortar for the first time, flatten the mortar with a pressure ruler, control the thickness of the cement mortar to 5mm, and cure for 60 minutes; apply the cement mortar for the second time, flatten the mortar with a pressure ruler, and control the cement mortar The thickness of the cement mortar is controlled at 5mm and cured for 60 minutes; the third time the cement mortar is applied, the mortar is flattened with a pressure ruler, and the thickness of the cement mortar is controlled at 8mm and cured for 48 hours;
[0057] S3 brushing super-hydrophobic emulsion: spray super-hydrophobic emulsion on the surface of the cured cement mortar, the dosage is 250g / m 2 , Cured for 7 days under the conditions of air humidity 75% ...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More