Plant planting vessel and manufacturing process thereof
A technology for making crafts and utensils, applied in the field of planting utensils and their making crafts, can solve the problems of energy-consuming materials, loss, plant withering, etc., and achieve the effects of increasing soil planting amount, light weight and beneficial to plant growth.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The manufacturing process of the plant planting vessel of the present embodiment comprises the following steps:
[0026] (1) Weigh 35% of cement, 33% of ceramsite, 3% of perlite, 17% of artificial sand, 10% of crystal soil, and 2% of 106 glue. After mixing evenly, add water. The amount of water added is 1 / 1 of the total amount of raw materials 5. Continue to stir until it reaches a uniform state. Among them, the crystal soil is crystal soil that has been fully swollen with clean water.
[0027] (2) The material obtained in step (1) is injected into a mold, cured at 25° C. for 12 hours, and shaped to obtain a plant planting vessel.
Embodiment 2
[0029] The manufacturing process of the plant planting vessel of the present embodiment comprises the following steps:
[0030] (1) Weigh 40% of cement, 33% of cinder, 3% of perlite, 15% of artificial sand, 7% of crystal soil, and 2% of 106 glue. After mixing evenly, add water. The amount of water added is 1 / 5 of the total amount of raw materials. , and continue stirring to a uniform state, wherein the crystal soil is crystal soil fully swelled by clear water.
[0031] (2) The material obtained in step (1) is injected into a mold, cured at 25° C. for 12 hours, and shaped to obtain a plant planting vessel.
Embodiment 3
[0033] The manufacturing process of the plant planting vessel of the present embodiment comprises the following steps:
[0034] (1) Weigh 45% of cement, 30% of ceramsite, 4% of perlite, 12% of quartz sand, 8% of crystal soil, and 1% of 106 glue. After mixing evenly, add water. The amount of water added is 1 / 1 of the total amount of raw materials 5. Continue to stir until it reaches a uniform state. Among them, the crystal soil is crystal soil that has been fully swollen with clean water.
[0035] (2) The material obtained in step (1) is injected into a mold, cured at 25° C. for 12 hours, and shaped to obtain a plant planting vessel.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com