Embodiment 1
[0030] A preparation method of a long-acting sleep-aiding latex pillow, comprising the following steps,
[0031] (1) Ingredients, pre-vulcanization
[0032] Prepare the raw materials according to the formula, and pre-cure them for 10 hours after stirring evenly. The raw materials are made of the following components by weight:
[0033] 100 parts of natural latex,
[0034] 7 parts of vulcanizing agent,
[0035] Potassium oleate 4 parts,
[0036] 1 part castor oil,
[0037] Potassium pyrophosphate 0.5 part,
[0038] 5 servings of sleep-promoting microspheres;
[0039] (2) Foaming the above-mentioned prevulcanized latex, adding 4 parts of zinc oxide and 2 parts of hardening agent in the foaming process;
[0040] (3) After steam vulcanization treatment at 100°C;
[0041] (4) The finished product is dried.
[0042] The preparation steps of the sleep aid microspheres are as follows: respectively weigh 1 part each of santalol, linalool, linalyl acetate and lavandulol, and 3 p...
Embodiment 2
[0044] A preparation method of a long-acting sleep-aiding latex pillow, comprising the following steps,
[0045] (1) Ingredients, pre-vulcanization
[0046] Prepare the raw materials according to the formula, and pre-vulcanize for 6 hours after stirring evenly. The raw materials are made of the following components by weight:
[0047] 100 parts of natural latex,
[0048] 4 parts of vulcanizing agent,
[0049] Potassium oleate 1 part,
[0050] 0.5 parts of castor oil,
[0051] Potassium pyrophosphate 0.1 parts,
[0052] 2 parts of sleep-promoting microspheres;
[0053] (2) Foaming the above-mentioned prevulcanized latex, adding 2 parts of zinc oxide and 4 parts of hardening agent in the foaming process;
[0054] (3) After steam vulcanization treatment at 100°C;
[0055] (4) The finished product is dried.
[0056] The preparation steps of the sleep-aiding microspheres are as follows: respectively weigh 2 parts of santalol, 3 parts of linalool, 3 parts of linalyl acetate,...
Embodiment 3
[0058] A preparation method of a long-acting sleep-aiding latex pillow, comprising the following steps,
[0059] (1) Ingredients, pre-vulcanization
[0060] Prepare the raw materials according to the formula, and pre-vulcanize for 15 hours after stirring evenly. The raw materials are made of the following components by weight:
[0061] 100 parts of natural latex,
[0062] 9 parts of vulcanizing agent,
[0063] Potassium oleate 6 parts,
[0064] 2 parts castor oil,
[0065] Potassium pyrophosphate 2 parts,
[0066] 8 servings of sleep aid microspheres;
[0067] (2) Foaming the above-mentioned prevulcanized latex, adding 10 parts of zinc oxide and 6 parts of hardening agent in the foaming process;
[0068] (3) After steam vulcanization treatment at 100°C;
[0069] (4) The finished product is dried.
[0070] The preparation steps of the sleep aid microspheres are as follows: respectively weigh 2 parts each of santalol, linalool, linalyl acetate, lavandulol and lac resin s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com