Water quality detection method for ocean lakes
A technology for water quality testing and lakes, applied in measuring devices, material analysis through electromagnetic means, instruments, etc., can solve the problems of further improvement of detection sensitivity, high detection cost, complex instruments, etc., to achieve improved catalytic ability and sensitivity, high The effect of electrocatalytic activity and mild synthesis conditions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0013] Add 0.1mol of butyl titanate, 0.1mol of zinc nitrate, 0.002mol of strontium nitrate, and 0.002mol of erbium chloride to 80ml of tert-butanol / glycerol mixed solution, the volume of tert-butanol / glycerol The ratio is 1:2, ultrasonically mixed evenly, then add 40ml of CTAB solution with a concentration of 0.3mg / mL, the volume ratio of tert-butanol / glycerol solvent to water is 1:0.5; after continuing to stir evenly, drop ammonia Aqueous solution, adjust the pH to 8; transfer it to a hydrothermal kettle, and conduct a hydrothermal reaction at 190 degrees Celsius for 12 hours to obtain Sr and Er co-doped TiO 2 -ZnO composite material;
[0014] Dissolve 0.1 mol of silver nitrate in water to obtain a silver nitrate solution, and then Sr, Er co-doped TiO 2 -ZnO composite material was added to the silver nitrate solution, followed by the introduction of 0.1 mol of reducing agent sodium citrate and 0.1 g of PVP, stirred and reacted at 80 degrees Celsius for 2 h to obtain Sr, Er c...
Embodiment 2
[0016] Add 0.1mol of butyl titanate, 0.1mol of zinc nitrate, 0.001mol of strontium nitrate, and 0.002mol of erbium chloride to 80ml of tert-butanol / glycerol mixed solution, the volume of tert-butanol / glycerol The ratio is 1:3, ultrasonically mix evenly, then add 40ml of CTAB aqueous solution with a concentration of 0.3mg / mL, the volume ratio of tert-butanol / glycerol solvent to water is 1:0.5; after continuing to stir evenly, drop ammonia aqueous solution, adjust the pH to 8; transfer it to a hydrothermal kettle, and conduct a hydrothermal reaction at 190 degrees Celsius for 18 hours to obtain Sr and Er co-doped TiO 2 -ZnO composite material;
[0017] Dissolve 0.1 mol of silver nitrate in water to obtain a silver nitrate solution, and then Sr, Er co-doped TiO 2 -ZnO composite material was added to the silver nitrate solution, followed by the introduction of 0.1 mol of reducing agent sodium citrate and 0.1 g of PVP, stirred and reacted at 80 degrees Celsius for 2 h to obtain Sr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com