Embodiment 1
[0018] A kind of colored clay crayon, adopts following steps to prepare:
[0019] Step 1, preparation of glue solution: under the temperature condition of 70°C, add 2 mass parts of polyvinyl alcohol and 30 mass parts of water to completely dissolve the polyvinyl alcohol in water, and keep stirring at this temperature for 1-4 hours. Then add 0.5 parts by mass of glycerin; finally add 8 parts by mass of silicone oil to obtain glue;
[0020] Furthermore, the polyvinyl alcohol and water are first soaked at room temperature for 1 hour, which makes it easier to dissolve.
[0021] Step 2, preparing synthetic wax: under the temperature condition of 70°C, melt 15 parts by mass of solid paraffin, 5 parts by mass of polyethylene wax and 4 parts by mass of stearic acid, add the melted synthetic wax to the glue, and Continue stirring for 2 h at the above temperature;
[0022] Step 3, preparing colored clay: adding 20 mass parts of calcium stearate to the above-mentioned synthetic wax, th...
Embodiment 2
[0025] A kind of colored clay crayon, adopts following steps to prepare:
[0026] Step 1, preparation of glue solution: at a temperature of 100°C, add 10 parts by mass of polyvinyl alcohol and 30 parts by mass of water to completely dissolve the polyvinyl alcohol in the water, and keep stirring at this temperature for 4 hours. Then add 2 mass parts of glycerin; finally add 6 mass parts of silicone oil to obtain glue;
[0027] Furthermore, the polyvinyl alcohol and water are first soaked at room temperature for 1 hour, which makes it easier to dissolve.
[0028] Step 2, preparing synthetic wax: under the temperature condition of 100°C, melt 15 parts by mass of paraffin wax, 4 parts by mass of polyethylene wax and 6 parts by mass of stearic acid, add the melted synthetic wax to the glue, and Continue stirring for 4h at the above temperature;
[0029] Step 3, preparation of colored clay: add 10 mass parts of calcium stearate to the above-mentioned synthetic wax, then add 10 mas...
Embodiment 3
[0031] A kind of colored clay crayon, adopts following steps to prepare:
[0032] Step 1, preparation of glue: at 90°C, add 8 parts by mass of polyvinyl alcohol and 20 parts by mass of water to completely dissolve the polyvinyl alcohol in water, and keep stirring at this temperature for 3 hours; then add 0.5 parts by mass of Parts of glycerin; Finally, add 8 parts by mass of silicone oil to obtain glue;
[0033] Furthermore, the polyvinyl alcohol and water are first soaked at room temperature for 1 hour, which makes it easier to dissolve.
[0034] Step 2, preparing synthetic wax: under the temperature condition of 90°C, melt 20 parts by mass of solid paraffin, 8 parts by mass of polyethylene wax and 6 parts by mass of stearic acid, add the melted synthetic wax to the glue, and Continue stirring for 3h at the above temperature;
[0035] Step 3, preparation of colored clay: Add 15 parts by mass of calcium stearate to the above-mentioned synthetic wax, then add 7 parts by mass ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com