A Melting Process for Reducing Shrinkage and Porosity in Ductile Iron
A technology of nodular cast iron and shrinkage porosity, which is applied in the direction of improving process efficiency, etc., can solve the problems of cast iron quality influence, small number of graphite balls, and shrinkage porosity of ductile iron, so as to improve strength and toughness, reduce production cost, and reduce internal The effect of shrinkage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A smelting process for reducing internal shrinkage of ductile iron, the steps of which are:
[0029] (1) Raw material preparation, preparation of return charge, scrap steel, recarburizer and ferrosilicon;
[0030] (2) The residual molten iron is kept in the intermediate frequency induction furnace, and the weight of the residual molten iron is 8% of the capacity of the intermediate frequency induction furnace. Add scrap to the intermediate frequency induction furnace with the residual molten iron, and the total weight of the scrap is 38% of the capacity of the intermediate frequency induction furnace. %, the scrap steel is added in three batches, each batch of scrap steel is added with a recarburizer, and the weight of the recarburizer added to the intermediate frequency induction furnace in each batch is 4% of the added scrap weight, which can make the scrap steel melt at the same time. Carbon agent, so that the recarburizer can be fully soaked and absorbed in the molt...
Embodiment 2
[0035] A smelting process for reducing internal shrinkage of ductile iron, the steps of which are:
[0036] (1) Raw material preparation, preparation of return charge, scrap steel, recarburizer and ferrosilicon;
[0037] (2) The residual molten iron soup is retained in the intermediate frequency induction furnace, and the weight of the residual molten iron soup is 12% of the capacity of the intermediate frequency induction furnace. Add scrap steel to the intermediate frequency induction furnace with the residual molten iron soup, and the total weight of the scrap steel is 42% of the capacity of the intermediate frequency induction furnace. %, the scrap steel is added in three batches, each batch of scrap steel is added with a recarburizer, and the weight of the recarburizer added to the intermediate frequency induction furnace in each batch is 4.2% of the added scrap steel weight, which can make the scrap steel melt at the same time. Carbon agent, so that the recarburizer can ...
Embodiment 3
[0042] A smelting process for reducing internal shrinkage of ductile iron, the steps of which are:
[0043] (1) Raw material preparation, preparation of return charge, scrap steel, recarburizer and ferrosilicon;
[0044] (2) The residual molten iron soup is retained in the intermediate frequency induction furnace, and the weight of the residual molten iron soup is 10% of the capacity of the intermediate frequency induction furnace. Add scrap steel to the intermediate frequency induction furnace with the residual molten iron soup, and the total weight of the scrap steel is 40% of the capacity of the intermediate frequency induction furnace. %, the scrap steel is added in three batches, each batch of scrap steel is added with a recarburizer, and the weight of the carburizer added to the intermediate frequency induction furnace in each batch is 4.1% of the added scrap steel weight, which can make the scrap steel melt at the same time. Carbon agent, so that the recarburizer can be...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com