[0023] Weigh 15.3 grams of PR254, 2.39 grams of PV23, 33.51 grams of PR101, and 1000 grams of CSC-B base material. Mix the above raw materials, and then apply the mixed composition evenly and evenly on the coated paper under the environmental conditions of relative humidity of 50%±5% and room temperature of 23±2°C. The wet film thickness of the coating is 250 μm, and then placed in a precision oven at 50±2°C for 3 to 4 hours to constant weight, taken out, cooled to room temperature, and obtained a physical color block.
Embodiment 2
[0025] Weigh 14.3 grams of PR254, 2.37 grams of PV23, 32.51 grams of PR101, and 1000 grams of CSC-B base material. Manufacturing process is with embodiment 1.
Embodiment 3
[0027] Weigh 16.3 grams of PR254, 2.38 grams of PV23, 3391 grams of PR101, and 1005 grams of CSC-B base material. Manufacturing process is with embodiment 1.