Preparation method of Pd complex compound loading catalyst
A technology for supporting catalysts and complexes, which is applied in the field of preparation of synthetic supported Pd complex catalysts, can solve the problems of high cost, and achieve the effects of mild synthesis conditions, high hydrogenation reaction activity, and cheap raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Suspend 2g of sodium bentonite (produced in Heishan, Liaoning) in 100ml of deionized water, stir at 50-60°C for 1 hour, add 1g of solid lysine hydrochloride therein, and carry out ion exchange reaction for 4 hours. Filter and wash with deionized water until Cl-free - . The solid was redispersed in 100ml of deionized water, stirred at 50-60°C for 1 hour, and 0.5ml of H 2 PdCl 4 Solution (Pd content is 20.035mg / ml), after dropwise addition, continue to react for 4 hours, filter, wash with deionized water until no Cl - . The obtained solid was dried at 70-80° C. for 4 hours. Grind the dried solid to - , that is, the supported Pd complex catalyst A is obtained.
Embodiment 2
[0020] The same as in Example 1, except that the catalyst B was prepared by using sodium Y-type molecular sieve.
Embodiment 3
[0022] The same as in Example 1, except that the catalyst C was prepared by using alumina calcined at 500° C. for 2 hours.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com