Method for preparing fire-resistant hydration-proof dolomite grog

A dolomite and waterproofing technology, applied in the field of dolomite clinker and its processing, can solve the problems of loss of use performance, difficulty in maintaining unbreakable, economic loss, etc., to simplify the production process, long service life, and solve problems of easy hydration. Effect

Inactive Publication Date: 2010-01-13
张广发
View PDF2 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, it is difficult to keep the above method unbreakable, and it is very easy to damage during use. If the protective film, wax layer, oil layer or packaging is broken, peeled off or opened, CaO, MgO particles or products are exposed to the atmosphere, and they will still be deliquescent, hydrated and crushed. Loss of performance, resulting in major economic losses

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] (1). The weight percentage is CaO20%, SiO 2 2 o 3 2 o 3 The raw dolomite ore with <0.5% is lightly burned at 1050-1100°C to obtain a product containing CaO and MgO, which is fully digested with water with a weight percentage of 43-45% for 48-50 hours to form a powder;

[0028] (2). After the digested dolomite powder obtained in step (1) is sieved through a sieve of 0.5-1.0mm, it is dried until the residual water is less than 1wt%, and then ground to be less than 0.074mm, that is, greater than 200 Purpose Dolomite light burnt powder is ready for use, sampling analysis, its chemical composition is: CaO35%, SiO 2 2 o 3 2 o 3 <0.5%;

[0029] (3). Get lightly burned dolomite powder 70Kg obtained in step (2) and add 30Kg lightly burned magnesium powder, its chemical composition is by weight percentage: CaO: 32.42%, MgO: 48.69%, SiO 2 : 1.01%, Fe 2 o 3 : 0.27%, Al 2 o 3 : 0.29%, according to the weight percentage plus SiO 2 , Fe 2 o 3 , CaF 2 , CeO 2 ,P 2 o 5 ...

Embodiment 2

[0036] (1). The weight percentage is CaO20%, SiO 2 2 o 3 2 o 3 The raw dolomite ore of <0.5% is lightly burned at 1100°C, and the obtained CaO and MgO products are fully digested with 44% water by weight for 48-50 hours, so that they are all powdered;

[0037] (2). After the digested dolomite powder obtained in step (1) is sieved through a sieve of 0.5-1.0mm, it is dried until the residual water is less than 1wt%, and then ground to be less than 0.074mm, that is, greater than 200 Purpose Dolomite light burnt powder is ready for use, sampling analysis, its chemical composition is: CaO35%, SiO 2 2 o 3 2 o 3 <0.5%;

[0038] (3). Get lightly burned dolomite powder 80Kg obtained in step (2) and add 20Kg lightly burned magnesium powder, its chemical composition is by weight percentage: CaO: 34.38%, MgO: 42.78%, SiO 2 : 0.41%, Fe 2 o 3 : 0.18%, Al 2 o 3 : 0.16%, according to weight percentage plus SiO 2 , Fe 2 o 3 , CaF 2 , CeO 2 ,P 2 o 5 and TiO 2 The binder of the...

Embodiment 3

[0045] (1). The weight percentage is CaO20%, SiO 2 2 o 3 2 o 3 The raw dolomite ore with less than 0.5% is lightly burned at 1050-1100°C, and the obtained CaO and MgO products are fully digested with water with a weight percentage of 43-45% for 48-50 hours, so that they are all powdered;

[0046] (2). After the digested dolomite powder obtained in step (1) is sieved through a sieve of 0.5-1.0mm, it is dried until the residual water is less than 1wt%, and then ground to be less than 0.074mm, that is, greater than 200 Purpose Dolomite light burnt powder is ready for use, sampling analysis, its chemical composition is: CaO35%, SiO 2 2 o 3 2 o 3 <0.5%;

[0047] (3). Get lightly burned dolomite powder 100Kg obtained in step (2), its chemical composition is by weight percentage: CaO: 43.72%, MgO: 31.19%, SiO 2 : 0.10%, Fe 2 o 3 : 0.10%, Al 2 o 3 : 0.07%, according to the weight percentage plus SiO 2 , Fe 2 o 3 , CaF 2 , CeO 2 ,P 2 o 5 and TiO 2 The binder of the co...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
densityaaaaaaaaaa
strengthaaaaaaaaaa
densityaaaaaaaaaa
Login to View More

Abstract

Disclosed is a process for preparing a heat resisting and hydration resisting clinker dolomite, relating to a treatment method for clinker dolomite. Lightly burning the dolomite ores, then sample analysis after fully digesting with water, sifting out, drying and milling, adding the wedding agent of external components according to weight percentages: SiO2 takes 8-13%, P2O5 takes 1-2%, CaF2 takes 1-1.5%, CeO2 takes 0.25-0.5%, Fe2O3 takes 1-3%, TiO2 takes 2-4%, dry blending the wedding agent via a sand mixer, then evenly mixing the wedding agent in the sand mixer, adding water and fully stirring the wedding agent to obtain a calendaring and moistureless mass, producing billets according to density which is similar to or more than 2.2g / cm3, then drying the wedding agent, the sintering curve is that lighting a fire and evenly heating up to 300 DEC G for 6-8 hours, and evenly heating up from 300 DEC G to 800 DEC G for 9-11hours, evenly heating up from 800 DEC G to 1200 DEC G for 6-8 hours, evenly heating up from 1200 DEC G to 1600 DEC G for 12-14 hours, sintering the wedding agent at a constant temperature of more than 1600 DEC G for not less than 8 hours, thereby achieving the heat resisting and hydration resisting clinker dolomite.

Description

technical field [0001] The invention relates to a dolomite clinker and a processing method thereof, in particular to a method for preparing high temperature-resistant and waterproof dolomite clinker. Background technique [0002] Dolomite is CaCO 3 · MgCO 3 or CaO·MgO·2(CO 2 ) double salt, which has high refractoriness and steel slag corrosion resistance, is an excellent raw material for the production of magnesia-calcium bricks, and has abundant reserves and low price. But since it was calcined at 1100°C, CO 2 After all of it is discharged, a mixture of MgO and CaO is formed. This mixture has a very low specific gravity, low mechanical strength, high porosity and chemical activity, and is very easy to absorb water and deliquescence to form Ca(OH) 2 and Mg(OH) 2 It will swell by itself, causing the particles to hydrate and break into powder, which cannot be used as a refractory material in production, thus losing its use value. For a long time, people have been making ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C04B2/10
CPCC04B2111/28C04B2/10C04B2111/27
Inventor 张广发
Owner 张广发
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products