Producing method of combing flax/richcel fiber blending high count yarn
A technology of lyssa fiber and flax fiber is applied in the production field of combed flax/lyssa fiber blended high-count yarn, which can solve the problems of difficult care and easy wrinkling of flax blended yarn, and achieve stable wearing performance and moisture absorption performance. Good, improve skin-friendly effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Embodiment 1: A kind of combed flax / Liesel fiber blended high-count yarn and its production method
[0022] According to the raw material ratio of the combed flax / Lysey fiber blended high-count yarn, 30% of the flax fiber and 70% of the Lisel fiber are weighed.
[0023] Production method:
[0024] a. Flax opening pretreatment process: The flax fiber weighed according to the proportion is opened and cleaned through the cotton picking machine, cotton mixer, cotton opener and cotton feeder, and then the processed flax fiber is processed. Spray emulsified oil accounting for 15% of the total amount of flax, stack it for more than 24 hours, and then pack it for use; the emulsified oil is prepared by emulsifying 0.8-1.3% spindle oil, 4.5-5.5% vegetable oil and water ;
[0025] b. The flax fiber that has been opened and pretreated is made into rolls through the cleaning process, and carded into raw sliver on the carding machine. The speed of the flat plate is 260-280mm / min, ...
Embodiment 2
[0030] Embodiment two: basically the same as embodiment one, the similarity is no longer described, and the difference is:
[0031] According to the raw material ratio of the combed flax / Lysey fiber blended high-count yarn, 32% of the flax fiber and 68% of the Lisel fiber are weighed.
[0032] In step a of the production method, the emulsified oil is added in an amount of 16% of the total amount of flax.
Embodiment 3
[0033] Embodiment three: basically the same as embodiment one, the similarity is no longer described, and the difference is:
[0034] According to the raw material ratio of the combed flax / Lysey fiber blended high-count yarn, 38% of the flax fiber and 62% of the Lisel fiber were weighed.
[0035] In step a of the production method, the amount of emulsified oil added is 17% of the total amount of flax.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More