Lightweight aggregate gypsum particle and production method thereof
A manufacturing method and technology of lightweight aggregates, which are applied in the field of lightweight aggregate gypsum particles and their manufacturing, can solve the problems of failing to meet architectural design indicators, sound insulation and thermal insulation effects, failing to meet building requirements well, and insufficient compressive strength. The effect of good sound insulation and heat preservation, light bulk density and low production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Mix 130 parts of raw material hemihydrate gypsum, 80 parts of light aggregate plant fiber, 2.2 parts of expanded plastic foam particles, 20 parts of Portland cement, and 300 parts of water, and then enter the screw extruder to make a diameter of 8-14 The granular shape of millimeters, after drying and curing for 3-5 days, it can become a finished product of light aggregate gypsum granules. For example, to manufacture 1 cubic meter of light aggregate gypsum particles, the raw materials are 130 kg of hemihydrate gypsum, 80 kg of light aggregate plant fiber, 2.2 kg of expanded plastic foam particles, 20 kg of Portland cement, and 300 kg of water.
Embodiment 2
[0018] Mix 140 parts of raw material hemihydrate gypsum, 100 parts of light aggregate plant fiber, 2 parts of expanded plastic foam particles, 25 parts of Portland cement, and 280 parts of water, and then artificially make particles with a diameter of 8-14 mm. shape, enter the dryer and bake at a temperature of 80-90°C for 12 hours, then it can be solidified and dried into finished products of light aggregate gypsum granules.
Embodiment 3
[0020] Mix 135 parts of the raw material hemihydrate gypsum, 180 parts of light aggregate fly ash, 7 parts of expanded perlite particles, 15 parts of Portland cement, and 250 parts of water, and then enter the screw extruder or roll into balls Machine into granules with a diameter of 8-14 mm, dry and solidify for 3-5 days, and then the light aggregate gypsum granules can be finished.
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com