Energy-saving and environmental-friendly medical injector and material for piston thereof
An energy-saving, environmentally friendly and injector technology, applied in hypodermic injection devices and other directions, can solve problems such as large consumption of raw materials, unfavorable production speed, and piston detachment from the core rod, and achieve the effect of reducing raw materials, reducing exhaust gas, and reducing thrust
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] Take 15 parts by weight of ethylene-vinyl acetate copolymer, 10 parts by weight of zinc stearate, 10 parts by weight of ethyl silicone oil with a viscosity of 20000, 10 parts by weight of ethyl silicone oil with a viscosity of 100, styrene-ethylene-butadiene- Put 50 parts by weight of styrene copolymer and 5 parts by weight of liquid paraffin into a high-speed stirrer, and stir for 10 to 50 minutes at room temperature to prepare a thermoplastic elastomer material, which is used for injection molding of pistons.
Embodiment 2
[0025] Take 10 parts by weight of ethylene-vinyl acetate copolymer, 5 parts by weight of zinc stearate, 10 parts by weight of ethyl silicone oil with a viscosity of 20000, 10 parts by weight of ethyl silicone oil with a viscosity of 100, styrene-ethylene-butadiene- Put 60 parts by weight of styrene copolymer and 5 parts by weight of liquid paraffin into a high-speed stirrer, and stir for 10 to 50 minutes at room temperature to prepare a thermoplastic elastomer material, which is used for injection molding of pistons.
Embodiment 3
[0027] Take 13 parts by weight of ethylene-vinyl acetate copolymer, 5 parts by weight of zinc stearate, 5 parts by weight of ethyl silicone oil with a viscosity of 20000, 5 parts by weight of ethyl silicone oil with a viscosity of 100, styrene-ethylene-butadiene- Put 70 parts by weight of styrene copolymer and 2 parts by weight of liquid paraffin into a high-speed stirrer, and stir for 10 to 50 minutes at room temperature to prepare a thermoplastic elastomer material, which is used for injection molding of pistons.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com