Preparation of low-carbon energy-saving modified polyethylene waterproof special material
A low-density polyethylene and polyethylene technology, applied in the field of polymer material preparation, can solve the problems of low elongation at break, high cost and low performance, and achieve the effects of large elongation at break, low cost and excellent performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Raise the temperature of the high-speed mixer to 60°C for standby; control the mixing temperature at 55-65°C during use. When mixing, control the speed at 800 rpm.
[0019] Weighing and mixing according to the designed modified polyethylene waterproof material formula. Weigh 130 kg of LDPE, 46 kg of LLDPE, and 20 kg of mLLDPE respectively, put them into a high-speed mixer that has been heated up, and mix for 5 minutes; then weigh 10 kg of maleic anhydride grafts and 1.0 kg of polyethylene wax lubricant, and add them to the In the high-speed mixer, mix for 5 minutes; finally weigh 5.2 kilograms of carbon black coloring agent, also add in the high-speed mixer, and mix for 15 minutes. The materials were mixed for about 25 minutes in total, and all the materials were mixed evenly for later use. The uniformly mixed spare material is continuously added to the material of the twin-screw extruder, and extruded, granulated, and packaged at a temperature of 130-190 ° C to obtai...
Embodiment 2
[0022] Raise the temperature of the high-speed mixer to 60°C for standby; control the mixing temperature at 55-65°C during use. The speed of mixing was controlled at 800 rpm.
[0023] Weighing and mixing according to the designed modified polyethylene waterproof material formula. Weigh 120 kg of LDPE, 30 kg of LLDPE, 20 kg of mLLDPE, and 24 kg of HDPE respectively, and put them into the high-speed mixer that has been heated up, and mix for 5 minutes; Put it into the high-speed mixer and mix it for 5 minutes; finally weigh 8.4 kg of carbon black, add it to the high-speed mixer, and mix it for another 15 minutes. The materials were mixed for about 25 minutes in total, and the materials were mixed evenly for later use. The uniformly mixed material is continuously fed into the twin-screw extruder, and melted, kneaded, extruded, granulated, and packaged at a temperature of 130-190 ° C to obtain a low-carbon energy-saving modified polyethylene waterproof material.
[0024] The pr...
PUM
Property | Measurement | Unit |
---|---|---|
oxidation induction time | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
elongation at break | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com