Embodiment 1
[0026] Fully dissolve 20 grams of polyvinylpyrrolidone powder (K90 grade) in 80 grams of water, and stir evenly to obtain polymer solution 1.
[0027] Dissolve 2.5 grams of polyurethane dispersion (R986, DSM) in 80 grams of deionized water, add 5 grams of polymer solution 1, stir evenly, add 0.15 grams of epoxy silane crosslinking agent, and continue stirring for 20 minutes.
[0028] Add 0.03 g of polyether-modified polysiloxane substrate wetting agent (Wet 245, Degussa) to the above solution, and continue stirring for 1 hour. The coating system can maintain good stability for a long time.
Embodiment 2
[0030] Fully dissolve 20 grams of polyvinylpyrrolidone powder (K90 grade) in 80 grams of water, and stir evenly to obtain polymer solution 1.
[0031] Dissolve 20 grams of polyurethane dispersion (R986, DSM) in 80 grams of deionized water, add 15 grams of polymer solution 1, stir evenly, add 0.6 grams of epoxy silane crosslinking agent, and continue stirring for 20 minutes.
[0032] Add 0.1 g of medical-grade polyether-modified silicon defoamer to the above solution, and continue stirring for 20 minutes. The coating system can maintain good stability for a long time.
Embodiment 3
[0034] Fully dissolve 20 grams of polyvinylpyrrolidone powder (K90 grade) in 80 grams of water, and stir evenly to obtain polymer solution 1.
[0035] Dissolve 20 grams of polyurethane dispersion (R986, DSM) in 70 grams of deionized water, add 25 grams of polymer solution 1, stir evenly, add 0.8 grams of epoxy silane crosslinking agent, and continue stirring for 20 minutes.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com