A technology of aerated bricks and ore pulp, applied in chemical instruments and methods, wet separation, manufacturing tools, etc., can solve problems such as polluting groundwater, affecting the life of iron oxide, environmental pollution, etc., and achieve the effect of increasing the service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0015] 1) Gold tailings processing: First, add water to the gold tailings and grind them in a ball mill to form a slurry with a particle size of more than 200 mesh. Gold tailings fine sand accounts for 70% of the slurry, and then extract the iron concentrate through a magnetic separator , put forward the ore pulp of iron concentrate and then extract sulfur concentrate through flotation machine, and obtain tailings after concentration and dehydration;
[0016] 2) Preparation of raw materials for aerated bricks: Mix and stir the tailings sand with lime, cement, water, and aluminum powder in proportions of 48%, 14%, 3%, 34.95%, and 0.05% by weight to obtain Aerated brick standard slurry;
[0017] 3), pouring the embryo body: pouring the prepared slurry into the brick mold to obtain the brick embryo body;
[0018] 4) Steaming the embryo body: put the embryo body in the steaming room for steaming, when the temperature of the steaming room is 50°C-60°C, the steaming time is 3-4 hou...